Lupolen 5261 Z Q 456 is a high density polyethylene (HDPE) with high melt viscosity for ram extrusion of peroxide crosslinked pipes (PE-Xa). The product is supplied as a nominal 20 mesh (840 µm) powder. It is not intended for medical or pharmaceutical applications. Processing Method: Extrusion Pipe, Sheet and Semi Finished Products. Physical Form: Powder. Typical Customer Applications: Plumbing, Heating and Cooling.This product is from the former Equistar product line. |