MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Arkema VOLTALEF® 302 PCTFE  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Polychlorotrifluoroethylene (PCTFE); Molded

Material Notes: VOLTALEF® 302 is a chlorotrifluoroethylene dense powder. Used in particular for compression molding, non-flammable.

Information provided by Arkema Group

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 2.11 - 2.16 g/ccASTM D1050-68
Apparent Bulk Density 1.00 g/cc
Particle Size 700 µm
Deformation 1.0 %7 MPa load for 24 hrs at 25°C; ASTM D621
 2.5 %7 MPa load for 24 hrs at 70°C; ASTM D621
 12 %7 MPa load for 24 hrs at 125°C; ASTM D621
 
Mechanical PropertiesOriginal ValueComments
Hardness, H358/30 80.0 MPaDIN 53456
Hardness, Shore D 75 - 90ASTM D676
Tensile Strength, Ultimate 32.0 - 40.0 MPaASTM D638
 13.0 - 16.0 MPa
@Temperature 120 °C
ASTM D638
Tensile Strength, Yield 34.0 - 50.0 MPaASTM D638
 3.00 - 6.00 MPa
@Temperature 120 °C
ASTM D638
Elongation at Break 100 - 250 %ASTM D638
Tensile Modulus 1.40 GPaASTM D638
Flexural Modulus 1.40 GPaASTM D790-80
Compressive Yield Strength 11.0 - 14.0 MPa1% deformation; ISO 604
 40.0 - 45.0 MPa0.2% off set; ISO 604
Compressive Modulus 1.40 GPaASTM D638
Izod Impact, Notched 0.800 J/cmASTM D256-81
Coefficient of Friction 0.26 - 0.45on polished steel
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.20e+18 ohm-cmASTM D257-78
Dielectric Constant 2.4 - 3.0
@Frequency 100 - 1.00e+8 Hz
ASTM D150
Dielectric Strength 15.0 kV/mm
@Thickness 3.20 mm
stepwise tension increase; ASTM D149-75
 21.0 kV/mm
@Thickness 1.60 mm
continuous tension; ASTM D149-75
 48.0 kV/mm
@Thickness 0.760 mm
stepwise tension increase; ASTM D149-75
 200 kV/mm
@Thickness 0.130 mm
stepwise tension increase; ASTM D149-75
Arc Resistance 360 secASTM D495-73
 
Thermal PropertiesOriginal ValueComments
CTE, linear 55.0 µm/m-°C
@Temperature -80.0 - 70.0 °C
ASTM D686-79
 250 µm/m-°C
@Temperature 70.0 - 150 °C
ASTM D686-79
Specific Heat Capacity 0.900 J/g-°C
Thermal Conductivity 0.135 W/m-KF 433
Maximum Service Temperature, Air 150 °Ccontinuous service
 200 °Cpeak
Oxygen Index 100 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polychlorotrifluoroethylene; Molded
DuPont Mobility and Materials VESPEL TP-8054 Polyimide
Overview of materials for Acetal Copolymer, Unreinforced
Overview of materials for Nylon 66, Unreinforced
Isoflon PCTFE Polychlorotrifluoroethylene

PARKG683 / 24531

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.