MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SK Chemicals SKYPET® BR8040 Low Content CHDM Modified Copolyester Resin
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: Description: SKYPET-BR8040 is a low content CHDM modified copolyester resin for large sized-mineral water bottles and extruded sheet. SKYPET-BR8040 has sufficiently low crystallization rate for large sized and refillable bottle of which preform is thicker than normal one. It also provides excellent processability in sheet extruding and thermoforming, especially deep drawing application, and has excellent chemical resistance for cosmetic containers.

Applications: Refillable bottles, 5 gallon water container, blister packaging for deep-draw application, heavy gauge sheets.

Information provided by SK Chemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.820 - 0.900 g/cc
Density 1.40 g/cc
Viscosity Test 78 - 82 cm³/gintrinsic viscosity
 
Thermal PropertiesOriginal ValueComments
Melting Point 234 - 238 °C
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.30 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SK Chemicals SKYPET® BL8050 Specially Formulated PET Copolymer Resin
SK Chemicals SKYPET® BB8055 Specially Formulated PET Resin
SK Chemicals SKYGREEN® PETG 2008 Specially Formulated PET Copolymer Resin
SK Chemicals SKYPET® XT8050 Specially Formulated PET Copolymer Resin
SK Chemicals SKYPET® BB7755 Specially Formulated PET Resin

PSK006 / 67741

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.