2-part, addition-curing silicone composition curing to a soft, tacky silicone adhesive. Low viscosity Special features: - highly biocompatible
- no by-products from curing process
- low viscosity, easily pourable
- 2-part, mixing ratio 1 : 1
- good adhesion
- high transparency
Application: SILPURAN® 2130 A/B can be used as a skin adhesive and for silicone sheets in medical applications.Information provided by Wacker Chemie AG. |