MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Industeel SIRIUS S12 20% Cr - 1.8% Si Heat Resistant Steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Description: CLI SIRIUS S12 grade is an austenitic stainless steel containing 20% Cr, 1.8 % Si and 12% Ni. The low nickel content combined with high chromium and high silicon contents provide good resistance to high temperature oxidation, even in sulphur containing gases The structure stability of the grade is enhanced compared to other more alloyed heat resistant steels. The alloy is designed to resist in oxidizing atmospheres up to 1000°C (1832°F). In cyclic conditions, a maximum temperature of 950°C (1742°F) should be considered. The alloy performs much better than 304 H and 304 N grades.

Information provided by manufacturer.

Key Words: EN 10095 X15 Cr Ni Si 20-12 - 1.4828, AFNOR Z10 CNS 20.12, DIN W. Nr 1. 4828, ASTM Type (302 B)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.90 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 540 MPaTypical after Solution Annealing
Tensile Strength, Yield 245 MPa
@Strain 0.2 %
Typical after Solution Annealing
 265 MPa
@Strain 1 %
Typical after Solution Annealing
Elongation at Break 40 %Typical
Creep Strength 140 MPa
@Temperature 600 °C,
Time 3.60e+6 sec
Modulus of Elasticity 200 GPa
Poissons Ratio 0.333Calculated
Shear Modulus 75.0 GPa
@Temperature 20.0 °C
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000900 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.0 µm/m-°C
@Temperature 20.0 - 100 °C
 17.0 µm/m-°C
@Temperature 20.0 - 200 °C
 18.0 µm/m-°C
@Temperature 20.0 - 400 °C
 18.5 µm/m-°C
@Temperature 20.0 - 600 °C
Specific Heat Capacity 0.500 J/g-°C
@Temperature 20.0 °C
Thermal Conductivity 15.0 W/m-K
@Temperature 20.0 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.10 %
Chromium, Cr 20 %
Iron, Fe 66.1 - 66.2 %As remainder
Nickel, Ni 12 %
Silicon, Si 1.8 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Architectural Bronze, UNS C38500
Industeel SIRIUS 314 25% Cr - 1.8% Si Heat Resistant Stainless Steel
Low-leaded brass, UNS C33500
Phosphor bronze 8% Sn, UNS C52100
Titanium, Ti

NINDUST27 / 17565

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.