MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
Aluminum 7475-T7351
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 7000 Series Aluminum Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: UNS A97475; ISO AlZn5.5MgCu(A); Aluminium 7475-T7351; AA7475-T7351; Al7475-T7351
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 2.81 g/ccAA; Typical
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 135500 kg load with 10 mm ball. Calculated value.
Hardness, Knoop 170Converted from Brinell Hardness Value
Hardness, Rockwell A 50.5Converted from Brinell Hardness Value
Hardness, Rockwell B 82Converted from Brinell Hardness Value
Hardness, Vickers 155Converted from Brinell Hardness Value
Tensile Strength, Ultimate 72.0 ksiAA; Typical
Tensile Strength, Yield 61.0 ksiAA; Typical
Elongation at Break 13 %
@Diameter 12.7 mm
AA; Typical
Modulus of Elasticity 10400 ksiAA; Typical; Average of tension and compression. Compression modulus is about 2% greater than tensile modulus.
Compressive Yield Strength 380 MPa0.1% Permanent Set
Poissons Ratio 0.33
Fatigue Strength 220 MPa
@# of Cycles 1.00e+7
Fracture Toughness 35.2 MPa-m½plate; S-L
 36.0 MPa-m½K(IC) in S-L Direction
 41.8 MPa-m½plate; T-L
 45.0 MPa-m½K(IC) in T-L Direction
 52.7 MPa-m½plate; L-T
 55.0 MPa-m½K(IC) in L-T Direction
Machinability 70 %0-100 Scale of Aluminum Alloys
Shear Modulus 27.0 GPa
Shear Strength 300 MPaCalculated value.
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 25.0 ohm-cir-mil/ft
@Temperature 20.0 °C
AA; Typical
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.9 µin/in-°F
@Temperature 20.0 - 100 °C
AA; Typical; average over range
 21.6 µm/m-°C
@Temperature -50.0 - 20.0 °C
 23.4 µm/m-°C
@Temperature 20.0 - 100 °C
 24.3 µm/m-°C
@Temperature 20.0 - 200 °C
 25.2 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.880 J/g-°CEstimated from trends in similar Al alloys.
Thermal Conductivity 1130 BTU-in/hr-ft²-°FAA; Typical at 77°F
Melting Point 890 - 1175 °FAA; Typical range based on typical composition for wrought products >= 1/4 in. thickness
Solidus 890 °FAA; Typical
Liquidus 1175 °FAA; Typical
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 775 °F
Solution Temperature 960 °Fmust be preceded by soak at 870 to 890°F
Aging Temperature 250 - 350 °F
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 88.5 - 91.5 %As remainder
Chromium, Cr 0.18 - 0.25 %
Copper, Cu 1.2 - 1.9 %
Iron, Fe <= 0.12 %
Magnesium, Mg 1.9 - 2.6 %
Manganese, Mn <= 0.06 %
Other, each <= 0.05 %
Other, total <= 0.15 %
Silicon, Si <= 0.10 %
Titanium, Ti <= 0.06 %
Zinc, Zn 5.2 - 6.2 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 7475-T61 (Extended High Temperature Data)
Aluminum 7039-T61
Titanium Ti-6Al-4V (Grade 5), Annealed
Aluminum 7475-T7651
Aluminum 7075-T6; 7075-T651

MA7475T735 / 9649

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.