MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Geon® Performance Solutions Vinyl Flexible XV3906 Polyvinyl Chloride, Flexible
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes:

NOTE: All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high water content only. This statement is only an overview of the FDA listings for this product. It is the customer's responsibility to ensure that the compound is suitable for its intended application. This compound has obtained conformance to Cytotoxicity tests under ISO 10993-5 GUIDELINES, when combined with Trans 1756 pigmentation.

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.21 g/cc1.21 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 757515 sec; ASTM D2240
Tensile Strength at Break 17.2 MPa2490 psiType IV, 510 mm/min; ASTM D638
Tensile Stress at Strain 8.27 MPa
@Strain 100 %
1200 psi
@Strain 100 %
Type IV, 510 mm/min; ASTM D638
Elongation at Break 350 %350 %Type IV, 510 mm/min; ASTM D638
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -35.0 °C-31.0 °FASTM D746
 
Compliance PropertiesMetricEnglishComments
FDA YesYesFood Contact, Unspecified Rating
 
Descriptive Properties
Agency RatingsCPSIA Compliant
 ISO 10993 Part 5
AppearanceClear/Transparent
FeaturesFood Contact Acceptable
 Non-Phthalate Plasticizer
FormsPellets
Generic MaterialPVC, Flexible
Generic NamePolyvinyl Chloride, Flexible
Processing MethodExtrusion
 Injection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesMedical Appliances

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution Luran® HD-20 SAN
Geon® Performance Solutions Vinyl Flexible XV3816 Polyvinyl Chloride, Flexible
Geon® Performance Solutions Vinyl Flexible XV 3450 Polyvinyl Chloride, Flexible

PH0POL1054 / 145623

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.