MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Ineos Nova 5751 High Impact Polystyrene  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: High flow, Good impact, USP Class VI

Applications: Single service impact, Medical, Housewares, Compounding

Properties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise specified.

Information provided by NOVA Chemicals.

INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets. 

Key Words: HIPS
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inASTM D955
Melt Flow 18 g/10 min18 g/10 minCondition G
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 22.0 MPa3190 psiASTM D638
Elongation at Break 35 %35 %ASTM D638
Flexural Yield Strength 39.0 MPa5660 psiASTM D790
Flexural Modulus 2.407 GPa349.1 ksiASTM D790
Izod Impact, Notched 0.800 J/cm
@Diameter 3.17 mm
1.50 ft-lb/in
@Diameter 0.125 in
bar, 0.010" notch radius; ASTM D256
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.51
@Frequency 1e+6 Hz
2.51
@Frequency 1e+6 Hz
Dielectric Strength 15.7 kV/mm
@Thickness 3.17 mm
400 kV/in
@Thickness 0.125 in
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 77.0 °C171 °FASTM D648
Vicat Softening Point 88.0 °C190 °FASTM D1525
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Melt Temperature 190 - 274 °C374 - 525 °F
Mold Temperature 38.0 - 82.0 °C100 - 180 °F
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution PS 5801 HIPS
Entec Hyrene® PS-HI 3/2 High Impact Polystyrene
Entec Hyrene® PS-HI 8/2 High Impact Polystyrene
Entec Hyrene® PS-HI 14/2 High Impact Polystyrene
Entec Hyrene® PS-HI 3/3 High Impact Polystyrene

PNOVA059 / 54960

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.