MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Industeel NUCL 18.10 B4 Natural Boron (Min 1% wt) Alloyed 304 Stainless Steel
Categories: Metal; Ferrous Metal; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Description: Isotope B10 has the property to capture neutrons produced by nuclear reactions. Natural boron contains about 19.9 at% or 18.45 wt % of B10 isotope, the remaining being B11 isotope. NUCL 18.10 B4 grade is a 304 stainless steel obtained by ingot casting and alloyed with 1 to 1,24 wt% natural boron additions. In order to avoid ferrite grain which reduce the ductility of the alloy, NUCL 18.10 B4 grade has been overalloyed in Nickel when compared to 304 grades. Molybdenum additions are sometimes considered to increase the corrosion resistance properties. The ingots rolled into plates are considered for nuclear applications (transport, casks, storage -in pools) of nuclear (waste) products. For specific purposes, some other grades are sometimes used. The boron content may thus be included in the 0.2-2 weight % range or/and alloys obtained by powder metallurgy (A type). CLI-FAFER can also produce 18-10 A or B type boron alloyed grades (included B10 enriched grades). Among the family of boron enriched 304 grades, NUCL 18-10 B4 grade is the most commonly used.

Information provided by manufacturer.

Key Words: aisi304, AISI 304, DIN W.14306 Bor-01 Ind.00, ASTM A887 UNS S30464 : Type 304B4, SUS304, SS304
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell <= 217Typical
Hardness, Rockwell B <= 95Typical
Tensile Strength, Ultimate >= 515 MPaMinimum Guaranteed
 610 MPaTypical
Tensile Strength, Yield >= 210 MPa
@Strain 0.2 %
 >= 225 MPa
@Strain 1 %
 310 MPa
@Strain 0.2 %
Typical
 325 MPa
@Strain 1 %
Typical
Elongation at Break >= 16 %
 19 %Typical
Modulus of Elasticity 200 GPa
Poissons Ratio 0.333Calculated
Shear Modulus 75.0 GPa
@Temperature 20.0 °C
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000950 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.0 µm/m-°C
@Temperature 20.0 - 100 °C
 17.5 µm/m-°C
@Temperature 20.0 - 200 °C
 18.0 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.500 J/g-°C
@Temperature 20.0 °C
Thermal Conductivity 15.0 W/m-K
@Temperature 20.0 °C
 
Component Elements PropertiesOriginal ValueComments
Boron, B 1.1 %
Carbon, C 0.013 %
Chromium, Cr 18.5 %
Iron, Fe 66.687 - 66.787 %As remainder
Manganese, Mn 0.80 %
Nickel, Ni 12.5 %
Nitrogen, N <= 0.10 %
Silicon, Si 0.30 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
304 Stainless Steel
Haynes Hastelloy® W alloy as a weld filler, base metal Type 304 Stainless steel 12.7 mm plate weldments
Kinetics MIM 316 Stainless Steel (Standard Grade)
AISI Type 304L Stainless Steel
Carpenter BioDur™ 316LS Stainless Medical Implant Alloy, Annealed

NINDUST35 / 17573

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.