MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Versalis Riblene® FF 29 Low Density Polyethylene - Blown Film Extrusion
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Riblene FF 29 is a high molecular weight low density polyethylene (LDPE), suitable for blown film extrusion. Riblene FF 29 is characterized by a good melt strength leading to a good bubble stability during extrusion.

Films manufactured with Riblene FF 29 are easily heat shrinkable and characterized by good mechanical properties.

Main Applications: Riblene FF 29 is recommended for the production of shrink film for medium loads, for agricultural film and for blends.

Information provided by Polimeri Europa.

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.921 g/ccISO 1183
Thickness 40.0 - 150 micronsRecommended
Melt Flow 0.60 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 10.0 MPaISO 527-3
Film Tensile Strength at Yield, TD 10.0 MPaISO 527-3
Film Elongation at Break, MD 400 %ISO 527-3
Film Elongation at Break, TD 600 %ISO 527-3
Coefficient of Friction, Dynamic >= 0.50ISO 8295
Elmendorf Tear Strength, MD 2.038 g/micronISO 6383-2
Elmendorf Tear Strength, TD 3.057 g/micronISO 6383-2
Dart Drop Test 310 gF50; ISO 7765-1
Film Tensile Strength at Break, MD 26.0 MPaISO 527-3
Film Tensile Strength at Break, TD 25.0 MPaISO 527-3
1% Secant Modulus, MD 160 MPaISO 527-3
1% Secant Modulus, TD 180 MPaISO 527-3
 
Thermal PropertiesOriginal ValueComments
Melting Point 111 °CInternal method
Vicat Softening Point 91.0 °C
@Load 1.00 kg
ISO 306/A
Brittleness Temperature <= -75.0 °CASTM D746
 
Optical PropertiesOriginal ValueComments
Haze 14 %ISO 14782
Gloss 45 %45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Versalis Riblene® GM 30 R Low Density Polyethylene - Coating Grade
Versalis Riblene® FF 24 Low Density Polyethylene - Blown Film Extrusion
Versalis Riblene® FF 22 Low Density Polyethylene - Blown Film Extrusion
Versalis Riblene® FF 20 Low Density Polyethylene - Blown Film Extrusion
Versalis Riblene® FC 40 Low Density Polyethylene - Blown Film Extrusion

PENG009 / 124403

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.