MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polyram PlusTek PA309G6 Nylon 6.6, 30% Glass Fiber
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: 30% glass fiber reinforced, UV stabilized polyamide 6.6 for injection molding applications

Information provided by Polyram Ram On Ind.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.37 g/ccDIN 53479
Water Absorption 5.6 %DIN 53495
Moisture Absorption at Equilibrium 1.7 %50%RH; DIN 53714
Linear Mold Shrinkage 0.0020 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 175 MPaASTM-D638
Elongation at Break 2.5 %ASTM-D638
Tensile Modulus 9.80 GPaASTM-D790
Flexural Strength 279 MPaASTM D790
Flexural Modulus 9.20 GPaASTM-D790
Izod Impact, Notched 1.10 J/cm
@Temperature 23.0 °C
ASTM-D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmDIN 53482
Surface Resistance 1.00e+12 ohmDIN 53482
Dielectric Constant 3.5
@Frequency 1e+6 Hz
VDE 0303/4
Dielectric Strength 90.0 kV/mmVDE 0303/4
 
Thermal PropertiesOriginal ValueComments
Melting Point 256 °C
Maximum Service Temperature, Air 120 °CContinuous Use
 240 °CShort peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 250 °CDIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 250 °CDIN 53461
Flammability, UL94 HB
@Thickness 3.00 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polyram PlusTek PA360G6 Nylon 6.6, 30% Glass Fiber
Polyram PlusTek PA301G6 Nylon 6.6, Heat Stabilized, 30% Glass Fiber
Polyram PlusTek PA305G6 Nylon 6.6, 30% Glass Fiber
Polyram PlusTek PA323G6 Nylon 6.6, 30% Glass Fiber, Flame Retardant
Polyram PlusTek PA325G6 Nylon 6.6, 30% Glass Fiber, Flame Retardant

PPOLYRA228 / 57490

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.