MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Desmopan® 9392A GMP TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Extrusion- and injection molding grade; very good hydrolysis and microbial resistance; good low-temperature flexibility; complies with VDE 0282-10; Application; Cable sheathings; Hoses, non-reinforced

Mechanical property data for samples at 50% RH.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.15 g/ccISO 1183-1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 92ISO 868
Hardness, Shore D 42ISO 868
Tensile Strength, Ultimate 7250 psi200 mm/min; b.o. ISO 527-1,-3
Tensile Stress at Strain 11.0 MPa
@Strain 100 %
200 mm/min; b.o. ISO 527-1,-3
 30.0 MPa
@Strain 300 %
200 mm/min; b.o. ISO 527-1,-3
Elongation at Break 400 %200 mm/min; b.o. ISO 527-1,-3
Tensile Modulus 71.0 MPa
@Temperature 60.0 °C
storage; ISO 6721-1,-4
 132 MPa
@Temperature 20.0 °C
storage; ISO 6721-1,-4
 700 MPa
@Temperature -20.0 °C
storage; ISO 6721-1,-4
Flexural Modulus 13.0 MPa
@Temperature 70.0 °C
Torsional storage; ISO 6721-2
 22.0 MPa
@Temperature 23.0 °C
Torsional storage; ISO 6721-2
 104 MPa
@Temperature -20.0 °C
Torsional storage; ISO 6721-2
Rebound 32 %Resilience; ISO 4662
Tear Strength 85.0 kN/m500 mm/min; ISO 34-1
Abrasion 20mm3; ISO 4649 method A
Compression Set 20 %
@Temperature 23.0 °C,
Time 259000 sec
ISO 815
 37 %
@Temperature 70.0 °C,
Time 86400 sec
DIN ISO 815-1, Method C
 55 %
@Temperature 70.0 °C,
Time 86400 sec
ISO 815
 
Processing PropertiesOriginal ValueComments
Melt Temperature 195 - 215 °CExtrusion
 210 - 230 °CInjection
Mold Temperature 20.0 - 40.0 °C
Drying Temperature 80.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Desmopan® 2792A GMP TPU
Covestro Desmopan® 9392AU Polyurethane
DSM Biomedical Bionate® II 55D Thermoplastic Polycarbonate Polyurethane (PCU)
Covestro Desmopan® 1092A TPU
AorTech Biomaterials Elast-Eon™ E2A Biomedical Polyurethane Pellets

PCOVEST0723 / 202506

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.