MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Michelman® Michem® Glide 37 Nonionic PTFE dispersion
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Description: Nonionic PTFE dispersion

Usage: Michem® Glide 37 as an additive provides mar, abrasion and high temperature resistance for a variety of applications within the paint and coating industries. Michem® Glide 37 also improves slip in coatings.

Typical uses include: Inks and OPVs; Exterior wood and wood composites and Interior furniture and flooring

Food Contact Information when manufactured in the USA:
FDA:
175.105: Components of adhesives
175.300: Resinous and polymeric components of coatings.
176.170: Components of paper and paperboard in contact with aqueous and fatty foods. (Restricted)
176.180: Components of paper and paperboard in contact with dry foods. (Restricted)

Food Contact Information when manufactured in Belgium:
FDA:
175.105: Components of adhesives.
176.170: Components of paper and paperboard in contact with aqueous and fatty foods. (Restricted)
176.180: Components of paper and paperboard in contact with dry foods. (Restricted)

Information provided by Michelman®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.45 - 1.47 g/cc
Volatiles 49.5 - 50.5 %
pH 3.0 - 7.0
 2.0 - 12Recommended pH of system
Brookfield Viscosity <= 5000 cPSpindle # 4, rpm 60
 
Descriptive Properties
AppearanceWhite, viscous liquid
Emulsifier ChargeNonionic
Solids TypePTFE

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Dyneon™ TF 5070GZ PTFE Dispersion
3M Dyneon™ TF 5033Z PTFE Dispersion
Daikin POLYFLON D-1E PTFE Dispersion
Chemours Teflon® PTFE 67 Resin for Lubricated Paste Extrusion
3M Dyneon™ TF 5235 PTFE Dispersion

WMICHEL125 / 135042

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.