MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis Borpact™ SG930MO Polypropylene Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Borpact™ SG930MO is a random heterophasic copolymer intended for injection molding. This grade yields high transparency and deep freeze impact resistance combined with excellent flow properties. and is designed for high-speed injection molding and contains nucleating and antistatic/demolding additives. In addition, components have good gloss, very low stress whitening and excellent taste and odor properties. Products molded from this grade have an excellent balance of see-through transparency and deep freeze impact resistance. Applications: ice cream containers, crates, deep freeze boxes for food storage, bread boxes, flip top caps, and high gloss closures.

Information provided by Borealis AG

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccISO 1183
Linear Mold Shrinkage 0.010 - 0.020 cm/cm
Melt Flow 25 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 18.0 MPa50mm/min; ISO 527-2
Elongation at Yield 15 %ISO 527-2
Tensile Modulus 850 MPa1mm/min; ISO 527-2
Charpy Impact, Notched 3.00 kJ/m²
@Temperature -20.0 °C
ISO 179/1eA
 11.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 69.0 °C
 
Processing PropertiesOriginal ValueComments
Melt Temperature 200 - 250 °C
Mold Temperature 15.0 - 40.0 °C
Hold Pressure 20.0 - 50.0 MPaminimize
 
Descriptive Properties
Injection Velocityhigh

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis BH345MO Polypropylene Copolymer
Borealis BD950MO Polypropylene Copolymer
Borealis RF926MO Polypropylene, Transparent Random Copolymer
Borealis BC918CF Polypropylene Copolymer
Borealis Borsoft™ SF203CF Soft Polypropylene Copolymer for Extrusion Coating

PBOREA383 / 108642

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.