MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Materion SupremEX® 640XA Aluminum - Silicon Carbide Metal Matrix Composite, T6 PGQ Forged Plate
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Aluminum Alloy; 6000 Series Aluminum Alloy

Material Notes: SupremEX® 640XA is an aluminum metal matrix composite (AA6061) that offers an extremely high tensile modulus (nearly double that of the parent alloy), good static and fatigue strengths well in excess of high performance aluminum alloys, while retaining reasonable ductility. This composite also demonstrates superior elevated temperature strength and thermal stability when compared with conventional aluminum alloys.

PGQ = Poly-Glycol Quench

Information supplied by Materion.

Key Words: AlSiC. Designation: – 6061/SiC/40p
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.90 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 76.9 ksi
Tensile Strength, Yield 58.0 ksi
@Strain 0.2 %
Elongation at Break 2.0 %
Modulus of Elasticity 140 GPa
Poissons Ratio 0.30
Shear Modulus 53.8 GPaCalculated
 
Thermal PropertiesOriginal ValueComments
CTE, linear 13.0 µm/m-°C
Specific Heat Capacity 0.800 J/g-°C
Thermal Conductivity 130 W/m-K
Melting Point >= 570 °C
Solidus 570 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Materion SupremEX® 640XA Aluminum - Silicon Carbide Metal Matrix Composite, T7 Forged Plate
Materion SupremEX® 640XA Aluminum - Silicon Carbide Metal Matrix Composite, T6 PGQ Billet
Materion SupremEX® 640XA Aluminum - Silicon Carbide Metal Matrix Composite, T6 CWQ Billet
Materion SupremEX® 217XG Aluminum - Silicon Carbide Metal Matrix Composite, T6 CWQ Forged Plate
MMCC Al/SiC Particulate Aluminum Matrix Composite

NBB9112 / 192333

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.