MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ovation Polymers Opnyl OP6GF33 Nylon 6, 33% Glass Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Nylon 6 - Glass reinforced (33 %), high tensile strength, stiffness and HDT.

*All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. For Nylon compounds the measurements are done in dry and wet conditions. All samples are prepared according to ASTM standards. Variations within normal tolerances are possible for various types of colors and functional properties like UV resistance.

Information provided by Ovation Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.40 g/cc1.40 g/ccASTM D792
Linear Mold Shrinkage 0.0015 - 0.0025 cm/cm
@Thickness 3.17 mm
0.0015 - 0.0025 in/in
@Thickness 0.125 in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 180 MPa26100 psi50 mm/min; ASTM D638
Elongation at Break 3.0 %3.0 %50 mm/min; ASTM D638
Tensile Modulus 9.00 GPa1310 ksi50 mm/min; ASTM D638
Flexural Yield Strength 230 MPa33400 psi1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 9.10 GPa1320 ksi1.3 mm/min; ASTM D790
Izod Impact, Notched 1.201 J/cm2.250 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
@Thickness 3.20 mm
421 °F
@Thickness 0.126 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 208 °C
@Thickness 3.20 mm
406 °F
@Thickness 0.126 in
ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman SCHULAMID® 6 GF33 33% Glass Fiber Reinforced Nylon 6
Ovation Polymers Nemcon™ H PK DP110/X5 Polyetheretherketone
Techmer ES HiFill® PA6 GF33 HS BK 33% Glass Filled
Ovation Polymers Opnyl OP66UT105 Nylon 66
Ovation Polymers Opnyl OP66GF13 Nylon 66, 13% Glass Reinforced

POVAT069 / 55781

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.