MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
FKuR Kunststoff Bio-Flex® F 1110 Compostable PLA Blend  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any starch or starch derivatives. Bioplastics generally replace conventional materials such as low density polyethylene (LDPE), high density polythene (HDPE) as well as polystyrene (PS) and polypropylene (PP). For packaging applications these materials need to be converted into film which is as thin as possible while maintaining high tensile strength. Depending on the specific application, packaging films have to provide a high barrier against humidity, oxygen and aromas or alternatively provide adequate permeability (“breathability”).

Information Provided by FKuR Kunststoff GmbH

Key Words: Polylactic Acid; biodegradable film
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.760 g/ccISO 60
Density 1.28 g/ccISO 1183
Melt Flow 2.0 - 4.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 16.0 MPaISO 527
Elongation at Yield >= 300 %ISO 527
Tensile Modulus 230 MPaISO 527
Flexural Strength 6.00 MPaat 3.5% strain; ISO 178
Flexural Modulus 215 MPaISO 178
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179-1/1eU
Charpy Impact, Notched NB
@Temperature 23.0 °C
ISO 179-1/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point >= 155 °CISO 3146-C
Vicat Softening Point 68.0 °CA; ISO 306
 
Descriptive Properties
Melt Volume Flow (cm3/10 min)1.5-3.5ISO 1133; 190°C, 2.16kg

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polylactic Acid (PLA) Biopolymer
FKuR Kunststoff Bio-Flex® A 4100 CL Compostable PLA Blend
FKuR Kunststoff Bio-Flex® F 1814 Compostable PLA Blend
FKuR Kunststoff Bio-Flex® F 2110 Compostable PLA Blend
FKuR Kunststoff Bio-Flex® F 2201 CL Compostable PLA Blend

PFKUR002 / 107040

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.