MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 1399 X 131270 C Polyphenylene Sulfide (PPS), Nickel-Coated Carbon Fiber - Electrically Conductive - EMI/RFI Shielding
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.77 g/cc1.77 g/ccASTM D 792
Linear Mold Shrinkage 0.00050 - 0.0010 cm/cm
@Thickness 3.17 mm
0.00050 - 0.0010 in/in
@Thickness 0.125 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 86.9 MPa12600 psiASTM D 638
Elongation at Break 0.20 - 0.50 %0.20 - 0.50 %ASTM D 638
Tensile Modulus 26.9 GPa3900 ksiASTM D 638
Flexural Strength 176 MPa25500 psiASTM D 790
Flexural Modulus 26.9 GPa3900 ksiASTM D 790
Izod Impact, Notched 0.534 J/cm
@Thickness 3.17 mm
1.00 ft-lb/in
@Thickness 0.125 in
ASTM D 256
Izod Impact, Unnotched 1.17 J/cm
@Thickness 3.17 mm
2.20 ft-lb/in
@Thickness 0.125 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1.0 ohm-cm<= 1.0 ohm-cmASTM D 257
Surface Resistance <= 1000 ohm<= 1000 ohmESD STM11.11
Surface Resistivity per Square <= 10000 ohm<= 10000 ohmASTM D 257
Static Decay <= 0.50 sec<= 0.50 secFTMS101C; 4046.1
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 238 °C460 °FASTM D 648
Flammability, UL94 V-0
@Thickness 1.59 mm
V-0
@Thickness 0.0625 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 307 - 329 °C585 - 625 °F
Mold Temperature 135 - 177 °C275 - 350 °F
Drying Temperature 149 °C
@Time 21600 sec
300 °F
@Time 6.00 hour
Moisture Content 0.040 %0.040 %
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company EMI 1363 Polyphenylene Sulfide (PPS), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
RTP Company EMI 1361 Polyphenylene Sulfide (PPS), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
RTP Company EMI 1262 S-80A Ester-based Thermoplastic Polyurethane Elastomer; Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding
RTP Company EMI 1063 Polybutylene Terephthalate (PBT); Stainless Steel Fiber - EMI/RFI Shielding - Electrically Conductive
RTP Company EMI 1062 Polybutylene Terephthalate (PBT), Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection

PQZTA23956 / 159219

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.