MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
PolyMirae Moplen EP440M Injection Molding Grade Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Moplen EP440M is the high isotacticity polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP440M is a block copolymer is typically used by customers for injection molding of battery case.

Product Features: Optimized balance of stiffness and toughness/High impact strength at low temperature/High Stiffness/Low warpage/High whiteness

Typical Applications: Battery case

Information provided by PolyMirae

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D1505
Melt Flow 9.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
Condition L; ASMT D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 97ASTM D785
Tensile Strength, Yield 280 kg(f)/cm²ASTM D638
Elongation at Yield 6.0 %ASTM D638
Flexural Modulus 12000 kg(f)/cm²ASTM D790
Izod Impact, Notched 4.00 kg-cm/cm
@Temperature -20.0 °C
ASTM D256
 10.0 kg-cm/cm
@Temperature 23.0 °C
ASTM D256

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Moplen EP440M Polypropylene, Impact Modified; Molded/Extruded
Bamberger Polymers Bapolene® 5010NB Polypropylene, Extrusion Grade
PolyMirae Moplen EP300L Injection Molding Grade Polypropylene
Aurora Plastics TufGuard M™ GPP1005M-EXLT PP, Flame Retardant
Aurora Plastics TufGuard M™ GPP1005M-CD PP, Flame Retardant

PMIRAF17 / 183238

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.