MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CeramTec Ziralit Zirconia Toughened Alumina (ZTA), Al2O3•ZrO2
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: CeramTec's Zirconia Toughened Alumina (Ziralit) provides excellent strength, excellent temperature performance, and superior toughness. It has enhanced performance for high quantity volume production and tight tolerances designs. Ziralit provides considerable improvement in strength and toughness over standard silicate products used in the fuse market. Due to its high temperature performance, the material has demonstrated successful application in the telecommunication fuse market where demanding requirements of 600V and 60A are typical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.80 g/cc
Water Absorption 0.00 %
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 200 GPa
Flexural Strength 335 MPa4 point
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.30e+7 ohm-cm
@Temperature 600 °C
 1.40e+13 ohm-cm
@Temperature 100 °C
 8.80e+15 ohm-cm
@Temperature 20.0 °C
Dielectric Strength 30.0 kV/mm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.60 µm/m-°C
@Temperature 20.0 - 200 °C
 8.20 µm/m-°C
@Temperature 20.0 - 500 °C
Specific Heat Capacity 0.800 J/g-°C
@Temperature 20.0 - 100 °C
Thermal Conductivity 13.0 W/m-K
@Temperature 20.0 - 100 °C
 
Descriptive Properties
ColorWhite
Thermal Shock Resistance R1 (K)130
Withstand Voltage (kV)> 15

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CeramTec 950 Zirconia Toughened Alumina (ZTA), Al2O3•ZrO2
CeramTec 977 Zirconia Toughened Alumina (ZTA), Al2O3•ZrO2
Astro Met ZTA 96 Zirconia Toughened Alumina
CeramTec 965 Toughened Alumina (Al2O3-ZrO2)
CeramTec ATZ Alumina Toughened Zirconia, Dental Grade

CCERA959 / 107559

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.