MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
I. Stern 728 High Gloss Medium Natural ABS  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Features:
  • Super high gloss
  • Easy to color

Applications

  • Injection molding
  • Appliances

Information provided by I. Stern & Co. Inc.

I. Stern & Co. Inc. has been acquired by Ravago.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccASTM D792
Melt Flow 11 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 111ASTM D785
Tensile Strength 7000 psiASTM D638
Elongation at Break 20 %ASTM D638
Flexural Strength 9950 psiASTM D790
Flexural Modulus 330000 psiASTM D790
Izod Impact, Notched 3.05 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Heat Distortion Temperature 187 °FASTM D648
Flammability, UL94 HB

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
I. Stern 750SW Medium Impact Natural ABS
I. Stern 745 Super High Impact Natural ABS
Multibase Multi-Pro® 2510 XGW High Gloss Polypropylene
Asahi Kasei Stylac™ 190F ABS Polymer, High Flow
Hannam Chemical Hanalac 780 ABS, High Flow

PISTER927 / 130887

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.