MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Danquinsa DANADD® FT-20/2000 Masterbatch
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: DANADD® FT-20/2000 is a high-quality flatting agent for thermoplastic polyurethanes (TPU’s). This additive masterbatch can be added to TPU types during their procession by injection moulding and extrusion. DANADD® FT-20/2000 is compatible with polyester-, co-polyether- and pure polyether TPU types. In addition to a high-grade flatting at the material surface, DANADD® FT-20/2000 is also used to obtain a reduced surface bonding and in some applications a better remoulding can be achieved in the injection moulding.

Application: DANADD® FT-20/2000 is added to our thermoplastic TPU ‘s for injection moulding and extrusion which are sold under the sales name PEARLTHANE®.. High-quality and matt-finished surfaces are obtained by adding this masterbatch. However, this special masterbatch can also be used in order to improve the extrusion- and injection moulding characteristics with regard to blocking resistance and surface-handle. DANADD® FT-20/2000 is a high-quality flatting Masterbatch which is also suitable for the 2Kinjection moulding and blow moulding.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.920 g/ccDIN 51.757
Storage Temperature 15.0 - 25.0 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 160 - 220 °C
Shelf Life 6.00 Month
 
Descriptive Properties
AspectWhite to yellowish regular (homogeneous) granules
Dosage1-10%
Heat resistance<230°C
Light resistanceLight scale up to scale no. 8

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDANQ004 / 294424

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.