MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultramid® A3HG5 BK00564 25% Glass Filled PA66 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Ultramid A3HG5 BK00564 is a 25% glass fiber reinforced injection molding PA66 grade.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.32 g/ccISO 1183
Water Absorption 5.7 - 6.3 %ISO 62
Moisture Absorption at Equilibrium 1.7 - 2.1 %23°C/50% R.H.; ISO 62
Viscosity Measurement 145ISO 307
Linear Mold Shrinkage 0.0055 cm/cm
Melt Flow 66 g/10 min
@Load 5.00 kg,
Temperature 275 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 170 MPaISO 527
Elongation at Yield 3.0 %ISO 527
Modulus of Elasticity 8.60 GPaISO 527
Flexural Strength 260 MPaISO 178
Flexural Modulus 7600 MPaISO 178
Izod Impact, Notched (ISO) 9.00 kJ/m²ISO 180/A
 9.50 kJ/m²
@Temperature -40.0 °C
ISO 180/A
Charpy Impact Unnotched 6.50 J/cm²ISO 179/1eU
 5.50 J/cm²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²ISO 179/1eA
 12.0 J/cm²ISO 179/1eA
 0.900 J/cm²
@Temperature -30.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmIEC 60093
Dielectric Constant 3.5
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.014
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 550 VTest Solution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 25.0 - 35.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359
CTE, linear, Transverse to Flow 60.0 - 70.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359
Specific Heat Capacity 1.60 J/g-°C
Thermal Conductivity 0.340 W/m-KDIN 52612
Melting Point 260 °CDIN 53765
Maximum Service Temperature, Air 140 °Cfor 50% loss of tensile strength after 20,000 hr
 170 °Cfor 50% loss of tensile strength after 5,000 hr
 240 °C
Deflection Temperature at 0.46 MPa (66 psi) 250 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 245 °CISO 75
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 - 300 °C
Mold Temperature 80.0 - 90.0 °C
 
Descriptive Properties
ColorBK00564
Commercial StatusNorth America and Europe
Impact ModifiedNo
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® A3HG2 10% Glass Filled PA66 (Dry)
BASF Ultramid® A3HG5 25% Glass Filled PA66 (Dry)
BASF Ultramid® A3HG5 25% Glass Filled PA66 (Conditioned)
BASF Ultramid® A3HG5 LS BK 23189 25% Glass Filled PA66 (Dry)
BASF Ultramid® A3HG5 LS BK 23189 25% Glass Filled PA66 (Conditioned)

PBASF9235 / 84999

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.