MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Lord Adhesives CoolTherm™ SC-320 SLW Thermally Conductive Silicone Encapsulant
Categories: Polymer; Thermoset; Silicone; Silicone Elastomer, for Thermal Management

Material Notes: CoolTherm™ SC-320 SLW thermally conductive silicone encapsulant is a two-component system designed to provide excellent thermal conductivity for electrical/electronic encapsulating applications, while retaining desirable properties associated with silicones.

Features: exhibits low shrinkage and stress on components as it cures. composed of an addition-curing polydimethyl siloxane polymer that will not depolymerize when heated in confined spaces. maintains low viscosity for ease of component encapsulation compared to other highly thermally conductive materials. provides excellent thermal shock resistance. provides excellent flame retardancy; UL 94 V-0 certified.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 3.10 g/ccSC-320 Resin
 3.10 g/ccSC-320 SLW Hardener
 3.10 g/ccMixed
Water Absorption <= 0.10 %cured; ASTM D 570-81
Viscosity 20000 cP
@Temperature 25.0 °C
SC-320 SLW Hardener
 22500 cP
@Temperature 25.0 °C
Mixed
 25000 cP
@Temperature 25.0 °C
SC-320 Resin
 
Chemical PropertiesOriginal ValueComments
Ionic Impurities - Na (Sodium) <= 10 ppmcured
Ionic Impurities - K (Potassium) <= 10 ppmcured
Ionic Impurities - Cl (Chloride) <= 10 ppmcured
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 24ASTM D 2240
Tensile Strength 36.0 psicured; ASTM D 412
Elongation at Break 40 %cured; ASTM D 412
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 4.00e+13 ohm-cm
@Temperature 25.0 °C
cured; ASTM D 257
 
Thermal PropertiesOriginal ValueComments
CTE, linear 110 µm/m-°Ccured; ASTM C 864
Thermal Conductivity 3.20 W/m-KHot Disc Transient Method, cured
Flammability, UL94 V-0
 
Processing PropertiesOriginal ValueComments
Working Life 180 min
@Temperature 25.0 °C
Mixed
Gel Time 20.0 min
@Temperature 120 °C
mixed
Shelf Life 9.00 Month
@Temperature 25.0 °C
each component from date of manufacture
 
Descriptive Properties
AppearanceLight Pink LiquidMixed
 Pink LiquidSC-320 Resin
 White LiquidSC-320 SLW Hardener
Extractable Ionic Contaminants10 ppm maxAmmonium
 10 ppm maxBromide
 10 ppm maxSulfate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Silicon Nitride
Silicon Nitride, HIP-RBSN
Silicon Nitride, HIP-SN
Silicon Nitride, HPSN
Silicon Nitride, RBSN

PLORD9293 / 232649

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.