MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® HexPly® M91 Epoxy Matrix
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: HexPly® M91 is a high performance, very tough epoxy matrix for use in aerospace primary structures and engines. HexPly® M91 is a toughened, controlled flow, epoxy resin system supplied with unidirectional fibers.

Benefits and Features

  • Excellent toughness with very high residual compression strength after impact.
  • Good translation of HexTow® fiber properties, both for intermediate modulus and high strength carbon fiber.
  • Designed for automation and particularly suited for both automated tape laying (ATL) and advanced fiber placement (AFP)
  • Good tack life and out-life, providing flexibility on the shop floor.
  • Low exotherm behavior allowing simple cures of thick monolithic structures up to 70mm (2.76”)
  • Dry Tg (DMA extrapolated onset E’) of 185°C-190°C (365°F-374°F)
  • Good hot-wet performance up to 120°C (250°F)

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 10000 cP
@Temperature 40.0 °C,
Time 2700 sec
Monolithic Part < 15mm (0.6inch) thick
 10000 cP
@Temperature 40.0 °C,
Time 4500 sec
Monolithic Part 15mm-70mm (2.7inch) thick
 1.00e+6 cP
@Temperature 120 °C,
Time 0.000 sec
Monolithic Part < 15mm (0.6inch) thick
 1.00e+6 cP
@Temperature 100 °C,
Time 0.000 sec
Monolithic Part 15mm-70mm (2.7inch) thick
 1.00e+7 cP
@Temperature 160 °C,
Time 4860 sec
Monolithic Part < 15mm (0.6inch) thick
 1.00e+8 cP
@Temperature 160 °C,
Time 15000 sec
Monolithic Part 15mm-70mm (2.7inch) thick
 
Processing PropertiesOriginal ValueComments
Gel Time 20.0 min
@Temperature 183 °C
 80.0 min
@Temperature 149 °C
 180 min
@Temperature 131 °C
Shelf Life 12.0 Month
@Temperature -18.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHEXCB9170 / 322326

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.