Daplen EE137AI is a 10% mineral filled grade intended for injection molding. EE137AI has been developed especially for the car industry, to be used in interior parts where high scratch resistance is a necessity. EE138AI offers good balance in stiffness/impact strength and has very good scratch resistance. Daplen EE137AI has been developed especially for dashboards, pillar trims, door panels and pockets, and other automotive interior parts. Information provided by the Manufacturer. |