MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Huntsman IROGRAN® A 80 P 4699L Ether-Based TPU-For Cable Industry
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Introduction: IROGRAN A 80 P 4699 L is a high performance polyether based thermoplastic polyurethane intended for extrusion and injection mold applications. IROGRAN A 80 P 4699 L is part of the HUNTSMAN extrusion / injection mold product range.

Performance Features:

  • Good melt flow
  • Low adhesion surface
  • High flexibility
  • Good processability
  • Soft

Information provided by Huntsman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.09 g/ccASTM D792
Linear Mold Shrinkage 0.0011 cm/cm
Melt Index of Compound 140 g/10 min
@Load 10.0 kg,
Temperature 190 °C
cm3/10 min
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80ASTM D2240
Tensile Strength at Break 30.0 MPaDIN 53504
Elongation at Break 670 %DIN 53504
100% Modulus 0.00570 GPa
@Strain 100 %
DIN 53504
300% Modulus 0.00840 GPa
@Strain 300 %
DIN 53504
Rebound 46 %Bayshore; ASTM D2632
Tear Strength 76.0 kN/mDIN 5315
Abrasion 50mm3; DIN 53516
Compression Set 24 %
@Temperature 23.0 °C,
Time 79200 sec
ASTM D395
 46 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395
 
Processing PropertiesOriginal ValueComments
Feed Temperature 175 °CExtrusion
Front Barrel Temperature 180 °CExtrusion
Adapter Temperature 180 °CExtrusion
Die Temperature 175 °CExtrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Huntsman IROGRAN® A 78 P 4766 NM Ether-Based TPU-For Cable Industry
Huntsman IROGRAN® A 75 P 4665N TPU-Polyether
Huntsman IROGRAN® A 80 P 5039 TPU-Polyether
Huntsman IROGRAN® A 85 P 4441 TPU-Polyether
Huntsman IROGRAN® A 85 P 4666 Ether-Based TPU-For Cable Industry

PHU9943 / 150403

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.