MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Naphthalene (C10H8)
Categories: Fluid; Solvent

Key Words: C10H8
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.0253 g/cc
@Temperature 20.0 °C
Molecular Weight 128.19 g/mol
Vapor Pressure 0.09869 atm
@Temperature 135.6 °C
 
Chemical PropertiesOriginal ValueComments
Critical Pressure 39.9704 atm
Critical Temperature 475.28 °C
Critical Density 0.315 g/cc
Critical Molar Volume 407 cm³/mol
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.54
@Temperature 85.0 °C
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 148.3 J/gEnthalpy of fusion at normal melting point
Heat of Vaporization 337 J/gEnthalpy of vaporization at normal boiling temperature
Melting Point 80.26 °CAt atmospheric pressure (760 torr)
Boiling Point 218 °C
@Pressure 0.101 MPa
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.4003
@Temperature 24.0 °C,
Wavelength 589.3 nm
Na D line

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Unipetrol Hydrogenated Refined Fermentative Ethanol Specially Denatured
Selenium, Se (alpha form)
Nitrogen, N2
NatureWorks® Ingeo™ 6201D Fiber Grade PLA
Michelman® Michem® Emulsion 71731MOD Anionic paraffin emulsion

VORG034 / 74545

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.