MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lubrizol LifeSciences Tecoflex® EG-93A-B40 TPU – 40% Barium Sulfate
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Medical Grade Aliphatic Polyether- based Thermoplastic Polyurethane (TPU) with 40% loading of Barium Sulfate

Features: offers an inherent ultraviolet (UV) stability that resists yellowing by aging and sterilization, good mechanical properties, radiopaque and can be color-matched

Process: Extrusion or Injection Molding

Key Words: BaSO4
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.52 g/ccASTM D792
Linear Mold Shrinkage 0.0060 - 0.010 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 95ASTM D2240
Tensile Strength, Ultimate 6500 psiASTM D412
Elongation at Break 430 %ASTM D412
100% Modulus 1400 psi
@Strain 100 %
ASTM D412
200% Modulus 2000 psi
@Strain 200 %
ASTM D412
300% Modulus 3100 psi
@Strain 300 %
ASTM D412
Flexural Modulus 4700 psiASTM D790
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 162.7 °CInjection
Front Barrel Temperature 162.7 °CInjection
Nozzle Temperature 168.3 °CInjection
Zone 1 171.1 °CExtrusion
Zone 2 176.6 °CExtrusion
Zone 3 182.8 °CExtrusion
Zone 4 187.7 °CExtrusion
Adapter Temperature 187.7 °CExtrusion
Die Temperature 187.7 °CExtrusion
Melt Temperature <= 196.1 °CInjection
Mold Temperature 10.0 - 37.7 °CInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol LifeSciences Tecoflex® EG-93A-B20 TPU – 20% Barium Sulfate
Lubrizol LifeSciences Carbothane® AC-4095A-B20 Aromatic TPU
Covestro Texin® RxT85A Thermoplastic Polyurethanes (TPU)
Lubrizol LifeSciences Carbothane® PC-3595A-B20 Aliphatic TPU
Lubrizol STAT-RITE® S-1100 Static Dissipative TPU

PLUBR9067 / 203634

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.