MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Plenco 7523 Phenolic, Granular, Transfer Molded  (discontinued **)
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic; Wood and Flock filled; Molded

Material Notes: PLENCO 07523 is a woodflour and cotton flock filled novolac phenolic molding compound, formulated for high impact industrial uses. UL recognized under component file E40654.

Information supplied by Plenco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.550 g/ccASTM D1895
Density 1.37 g/ccASTM D792
Water Absorption 0.40 %ASTM D570
Linear Mold Shrinkage 0.0079 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell E 84ASTM D785
Tensile Strength, Ultimate 53.0 MPaASTM D638
Elongation at Break 0.82 %ASTM D638
Tensile Modulus 7.50 GPaASTM D638
Flexural Strength 68.0 MPaASTM D790
Flexural Modulus 6.80 GPaASTM D790
Compressive Strength 194 MPaASTM D695
Izod Impact, Notched 19.2 J/mASTM D256
Charpy Impact, Notched 0.199 J/cm²ASTM D256
Impact 118J/m Drop Ball Impact; PLENCO
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.80e+11 ohm-cmASTM D247
Dielectric Constant 4.9ASTM D150
Dielectric Strength 10.9 kV/mmShort Time; ASTM D149
Dissipation Factor 0.054ASTM D150
Arc Resistance 133 secASTM D495
Comparative Tracking Index 150 VASTM D3638
 
Thermal PropertiesOriginal ValueComments
CTE, linear 60.0 µm/m-°C
@Temperature 40.0 - 130 °C
TMA; ASTM E831
Maximum Service Temperature, Air 200 °CHeat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 158 °CASTM D648
Flammability, UL94 HB
@Thickness 1.50 mm
Shrinkage 0.267 %72 hr, 120ºC; ASTM D1299

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
European Horse Chestnut Wood
European Bastralocus Wood
DIAB ProBalsa® LD7 Light Weight Balsa Wood
CoreLite BALSASUD® Core UL Ultra Lite Balsa Core Material
Carbon-Core Carbon Balsa Wood

PLEM46 / 50727

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.