MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Huntsman IROGRAN® A 78 E 4723 Polyester-Based TPU-Injection Extrusion Grade
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: Introduction: IROGRAN A 78 E 4723 is a thermoplastic polyester- polyurethane for injection moulding and extrusion applications. Additional characteristics of the product are flexibility and high mechanical resistance.

Performance Features:

  • High transparence
  • Good melt flow
  • High wear resistance
  • High oil resistance
  • Dynamically highly loadable
Applications: For the production of spiral hoses, profiles hoses, jackets for high pressure hoses, technical parts.

Information provided by Huntsman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccASTM D792
Linear Mold Shrinkage 0.0080 in/inASTM D995
Melt Index of Compound 50 g/10 min
@Load 21.6 kg,
Temperature 190 °C
cm3/10 min
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80ASTM D2240
Hardness, Shore D 30ASTM D2240
Tensile Strength at Break 45.0 MPaDIN 53504
Elongation at Break 660 %ASTM D412
100% Modulus 0.00410 GPa
@Strain 100 %
DIN 53504
300% Modulus 0.0100 GPa
@Strain 300 %
DIN 53504
Rebound 47 %Bayshore; ASTM D2632
Tear Strength 510 pliASTM D624
Abrasion 25[mm3]; ISO 4649
Compression Set 25 %
@Temperature 23.0 °C,
Time 252000 sec
ASTM D395
 38 %
@Temperature 70.0 °C,
Time 86400 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
Melting Point 156 - 167 °CHuntsman/TMA
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %transparent; thickness not reported
 
Processing PropertiesOriginal ValueComments
Feed Temperature 25.0 - 40.0 °CExtrusion
Front Barrel Temperature 165 - 190 °CExtrusion
Nozzle Temperature 170 - 200 °CExtrusion
 180 - 200 °CInjection
Adapter Temperature 175 - 195 °CExtrusion
Die Temperature 175 - 200 °CExtrusion
Melt Temperature 170 - 195 °CInjection
Mold Temperature 20.0 - 70.0 °CInjection
 
Descriptive Properties
Heating Zone175-195°CInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Huntsman IROGRAN® A 92 E 4694 Polyester-Based TPU-Injection Extrusion Grade
Huntsman IROGRAN® A 95 E 4813 Polyester-Based TPU-High Performance Grade
Covestro Desmopan® 2590A Thermoplastic Polyurethane
Covestro DUREFLEX® U04 TPU
Lubrizol Advanced Materials PEARLTHANE® Clear 15N85 Thermoplastic Polyurethane Elastomer

PHU9913 / 150373

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.