MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Spartech Polycast Poly 2000 (Mil-P-25690;Class 2) Cell Cast Acrylic
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Cast

Material Notes: Description: Cell Cast Acrylic

Information provided by Spartech.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/ccASTM D792
Water Absorption 0.20 %24 hr immersion
Water Absorption at Saturation 1.6 %26 day immersion
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 12100 psiASTM D638
Shear Strength 3700 psiASTM D732
 
Thermal PropertiesOriginal ValueComments
CTE, linear 42.0 µin/in-°F
@Temperature 20.0 °C
ASTM D696
Specific Heat Capacity 0.350 BTU/lb-°F
@Temperature 25.0 °C
Dupont 900 (Therm. An. Cal.)
Thermal Conductivity 1.30 BTU-in/hr-ft²-°FCento-Fitch
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.49ASTM D542
Haze <= 1.5 %As Cast; ASTM D1925
 <= 3.0 %After 1000 hrs. Accelerated Weathering; ASTM D1449
Transmission, Visible 90 %After 1000 hrs. Accelerated Weathering; ASTM D1449
 91 %As Cast; ASTM D1003
 
Processing PropertiesOriginal ValueComments
Processing Temperature 218 °FHot Forming Temperature
 
Descriptive Properties
Crack Propagation2900 lbs/in 3/2Received at STD Conditions
Craze Resistance to IPA (Dry)4300 psiMil-P-8184
Craze Resistance to IPA (Wet)3600 psiMil-P-8184
Craze Resistance to Lacquer Thinner (Dry)3600 psiMil-P-8184
Craze Resistance to Lacquer Thinner (Wet)3000 psiMil-P-8184
Thermal Relaxation at 230°F3.3 %Mil-P-25690
Thermal Relaxation at 293°F45 %Mil-P-25690

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Spartech Polycast Poly 2000 (Mil-P-25690;Class 1) Cell Cast Acrylic
Spartech Polycast Poly 76 (Mil-P-8184) Cell Cast Acrylic
Spartech Polycast Poly 84 (Mil-P-8184) Cell Cast Acrylic
Spartech Polycast Poly 900 (DTD-5592-UK) Cell Cast Acrylic
Titanium Ti-6Al-4V (Grade 5), Annealed

PSPAR032 / 68473

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.