MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Go Yen Chemical Goyenchem-HIPS27 High Impact Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Characteristic:
  • Super High Impact Extrusion Grade
  • Super High Impact Strength
  • Low Residual Monomer
  • Good Heat Resistance
  • Base Color Stability
  • Excellent Transparency
  • Easy Processing
  • High Flow
Applications: Extruded sheets, cable reels, buoy

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccASTM D792
Melt Flow 2.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 99ASTM D785
Tensile Strength, Yield 25.5 MPa
@Thickness 3.17 mm
ASTM D638
Elongation at Break 45 %
@Thickness 3.17 mm
ASTM D638
Flexural Yield Strength 470 kg(f)/cm²
@Load 1.00 kg,
Thickness 3.00 mm
120°C/h; ASTM D790
Flexural Modulus 2060 MPa
@Load 1.00 kg,
Thickness 3.00 mm
120°C/h; ASTM D790
Izod Impact, Notched 88.2 J/mA method, 1/4”×1/2”×5/2”; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 89.0 °C
@Thickness 12.7 mm
Unannealed; ASTM D648
Vicat Softening Point 102 °C
@Load 1.00 kg,
Thickness 3.00 mm
120°C/h; ASTM D1525
 
Processing PropertiesOriginal ValueComments
Processing Temperature 160 - 280 °CCylinder
Mold Temperature 35.0 - 65.0 °C
Injection Pressure 49.0 - 137 MPa
 
Descriptive Properties
Composition800 ppmResidual SM monomer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOYEN786 / 267094

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.