MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Gouda Refractories Pinnacle PP 2160H PP Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Product Description: 65 melt flow impact copolymer for injection molding. Pinnacle Polymers Polypropylene 2160H is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties and lot-to-lot consistency. This controlled rheology copolymer is intended for use in thin wall injection molded packaging, housewares and consumer products applications. High Melt Flow improves cycle-times without forfeiting impact. Contains nucleator and antistat.
Features: High stiffness; Excellent impact 23°C and -30°C; Very high melt flow; Excellent mold release; Superior processability; Excellent lot-to-lot consistency; UL Listed
Pinnacle’s 2160H polypropylene as marketed by Pinnacle Polymers Company, in natural, uncolored pellet form is covered under US FDA Food Contact Notification 864. As such, this polymer complies with the requirements of CFR Title 21 and can be used in contact with all food types under Conditions of Use A-H.

Availability: Europe; North America

Additive: Antistatic; Nucleating Agent

Features: Antistatic; Controlled Rheology; Food Contact Acceptable; Good Mold Release; Good Processability; High Flow; High Impact Resistance; High Stiffness; Impact Copolymer; Low Temperature Impact Resistance; Nucleated

Agency Ratings: FDA FCN 864; FDA Food Contact Tables 1 &2, Cond A-H; UL

Appearance: Natural Color

Form: Pellets

Processing Method: Injection Molding

Information provided by Pinnacle Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D1505
Linear Mold Shrinkage, Flow 0.013 cm/cm0.013 in/inASTM D955
Melt Flow 65 g/10 min
@Load 2.16 kg,
Temperature 230 °C
65 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 26.9 MPa
@Thickness 3.20 mm
3900 psi
@Thickness 0.126 in
Injection Molded, Type I, 2.0 in/min; ASTM D638
Elongation at Break 5.0 %
@Temperature -17.7 °C
5.0 %
@Temperature 0.126 °F
Injection Molded, Type I, 2.0 in/min; ASTM D638
Flexural Modulus 1.36 GPa
@Thickness 3.20 mm
197 ksi
@Thickness 0.126 in
1% Secant, Injection Molded, Type I, 0.05 in/min; ASTM D790A
Izod Impact, Notched  0.747 J/cm
@Thickness 3.20 mm
1.40 ft-lb/in
@Thickness 0.126 in
Injection Molded, Type I; ASTM D256
 1.85 J/cm
@Thickness 3.20 mm
3.47 ft-lb/in
@Thickness 0.126 in
(Area) Injection Molded, Type I; ASTM D256
Gardner Impact 11.0 J
@Temperature -30.0 °C
8.12 ft-lb
@Temperature -22.0 °F
Geometry GC, Method G; ASTM D5420
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 115 °C239 °FUnannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPINNA823 / 311516

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.