MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chesterton ARC 982 100% Novolac acid resistant coating  (discontinued **)
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: An advanced polymer composite formulated to protect equipment from extreme chemical attack and corrosion. A low viscosity composite that is applied by brush, squeegee, or a plural component sprayer system. ARC 982 may be applied at a minimum thickness of 250 microns (10 mils) per coat. A two-coat application of ARC 982 provides protection from concentrated acids, alkailes, and solvents. The cured composite provides outstanding chemical resistance with a high gloss finish.

Benefits:

  • Excellent resistance to a wide variety of concentrated acids such as sulfuric acid up to 98% and fluctuating chemical environments.
  • ARC 982 outlasts rubber and other traditional lining materials as it is resistant to aging and embrittlement
  • Tough resin structure resists thermal-mechanical shock
  • Outstanding adhesion results in reliable performance with no under film corrosion
  • Holiday testable per NACE RP0188

Suggested Uses:

  • Chemical Storage Tanks
  • Exhaust Gas Ductwork
  • Impellers
  • Pump Casings
  • Structural Steel
  • Valves
  • Chimneys and Stacks
  • Fans and Housings
  • Heat Exchangers
  • Tanks and Piping
  • Reaction Vessels

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³Cured
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8282ASTM D2240
Elongation at Break 1.1 %1.1 %ASTM D638
Flexural Strength 30.6 MPa4440 psiASTM D790
Flexural Modulus 3.24 GPa470 ksiASTM D790
Compressive Strength 85.56 MPa12410 psiASTM D695
Adhesive Bond Strength >= 19.0 MPa>= 2750 psiASTM D4541
Impact Test 2.49 J1.83 ft-lbReverse; ASTM D2794
 3.16 J2.33 ft-lbDirect; ASTM D2794
 
Thermal PropertiesMetricEnglishComments
CTE, linear 102 µm/m-°C56.9 µin/in-°FASTM C531
Maximum Service Temperature, Air 70.0 °C158 °FWet Service
 175 °C347 °FDry Service
 
Processing PropertiesMetricEnglishComments
Cure Time  360 min
@Temperature 32.0 °C
6.00 hour
@Temperature 89.6 °F
Light Load/Overcoat End
 600 min
@Temperature 25.0 °C
10.0 hour
@Temperature 77.0 °F
Light Load/Overcoat End
 1200 min
@Temperature 16.0 °C
20.0 hour
@Temperature 60.8 °F
Light Load/Overcoat End
 1200 min
@Temperature 32.0 °C
20.0 hour
@Temperature 89.6 °F
Full Load
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Full Load
 1800 min
@Temperature 10.0 °C
30.0 hour
@Temperature 50.0 °F
Light Load/Overcoat End
 2880 min
@Temperature 16.0 °C
48.0 hour
@Temperature 60.8 °F
Full Load
 4320 min
@Temperature 10.0 °C
72.0 hour
@Temperature 50.0 °F
Full Load
 10100 min
@Temperature 32.0 °C
168 hour
@Temperature 89.6 °F
Chemical Resistance
 17300 min
@Temperature 25.0 °C
288 hour
@Temperature 77.0 °F
Chemical Resistance
 20200 min
@Temperature 16.0 °C
336 hour
@Temperature 60.8 °F
Chemical Resistance
 25900 min
@Temperature 10.0 °C
432 hour
@Temperature 50.0 °F
Chemical Resistance
Tack-Free Time  300 min
@Temperature 32.0 °C
5.00 hour
@Temperature 89.6 °F
 480 min
@Temperature 25.0 °C
8.00 hour
@Temperature 77.0 °F
 960 min
@Temperature 16.0 °C
16.0 hour
@Temperature 60.8 °F
 1440 min
@Temperature 10.0 °C
24.0 hour
@Temperature 50.0 °F
 
Descriptive Properties
ColorLight Gray
 Medium Gray

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lehvoss LUVOCOM® 1301/GF/30/TF/15 PPS, linear with glass fiber and PTFE
Chesterton ARC 855 Abrasion Control Coating
Supreme Petrochem SP 253 Toughened Polystyrene
Saint-Gobain Tygon® A-60-G Industrial Grade Tubing Formulation
Prodways PLASTCure Pattern 2500 Liquid Resin for 3D Printing

PPTCHS033 / 138145

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.