MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Envalior Akulon® K224-HG8 PA6-GF40, Dry, 40% Glass Filled, Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 40% Glass Fiber Filled; Nylon 6, Heat Stabilized

Material Notes: 40% Glass Reinforced, Heat Stabilized

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.45 g/ccISO 1183
Water Absorption 5.5 %Sim. ISO 62
Moisture Absorption 1.70 %Humidity; Sim. ISO 62
Linear Mold Shrinkage, Flow 0.0034 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0083 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 205 MPaISO 527-1/-2
Elongation at Break 3.0 %ISO 527-1/-2
Tensile Modulus 13000 MPaISO 527-1/-2
Flexural Strength 275 MPaISO 178
Flexural Modulus 10800 MPaISO 178
Charpy Impact Unnotched 85.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
 95.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 13.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 18.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cmIEC 60250
Dielectric Constant 3.3
@Frequency 1e+6 Hz
IEC 60250
 3.5
@Frequency 100 Hz
IEC 60250
Dielectric Strength 35.0 kV/mmIEC 60243-1
Dissipation Factor 0.0050
@Frequency 100 Hz
IEC 60250
 0.015
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 50.0 µm/m-°CISO 11359-1/-2
Melting Point 220 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 220 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 200 °CISO 75-1/-2
Flammability, UL94 HB
@Thickness 1.50 mm
IEC 60695-11-10
 HB
@Thickness 0.710 mm
IEC 60695-11-10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior Akulon® K224-HG8 PA6-GF40, Conditioned, 40% Glass Filled, Heat Stabilized
Envalior Akulon® F223-D PA6, Dry, Low/Medium Viscosity
Envalior Akulon® K224-LGM35 (Cond.) 15% Glass Reinforced, 25% Mineral Reinforced Nylon 6 (North America)
RTP Company RTP 899 X 131271 A Acetal (POM), High Purity - Wear Resistant
Envalior Akulon® K224-G6 PA6-GF30, Dry, 30% Glass Filled

PDSM8049 / 184750

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.