MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Bayblend® M750 PC/ABS Blend
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: (PC+ABS)-Blend; Vicat/B 120 temperature = 126 °C; meet certain requirements of ISO Standard 10993-1.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³ISO 1183-1
Moisture Absorption at Equilibrium 0.20 %0.20 %ISO 62
Water Absorption at Saturation 0.60 %0.60 %ISO 62
Viscosity 265000 cP
@Frequency 1000 Hz,
Temperature 260 °C
265000 cP
@Frequency 1000 Hz,
Temperature 500 °F
Melt; b.o. ISO 11443-A
Linear Mold Shrinkage, Flow 0.0070 - 0.0090 cm/cm0.0070 - 0.0090 in/in150x105x3 mm; 260 °C / MT 80 °C; b. o. ISO 2577
Linear Mold Shrinkage, Transverse 0.0070 - 0.0090 cm/cm0.0070 - 0.0090 in/in150x105x3 mm; 260 °C / MT 80 °C; b. o. ISO 2577
Melt Flow 12.32 g/10 min
@Load 5.00 kg,
Temperature 260 °C
12.32 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 47.0 MPa6820 psi50 mm/min; ISO 527-1,-2
Elongation at Break >= 50 %>= 50 %Nominal, 50 mm/min; ISO 527-1,-2
Elongation at Yield 4.8 %4.8 %50 mm/min; ISO 527-1,-2
Tensile Modulus 2.00 GPa290 ksi1 mm/min; ISO 527-1,-2
Izod Impact, Notched (ISO)  35.0 kJ/m²
@Temperature -30.0 °C
16.7 ft-lb/in²
@Temperature -22.0 °F
ISO 180-A
 45.0 kJ/m²
@Temperature 23.0 °C
21.4 ft-lb/in²
@Temperature 73.4 °F
ISO 180-A
Izod Impact, Unnotched (ISO) NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 180-U
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 85.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
47.2 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1, -2
CTE, linear, Transverse to Flow 85.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
47.2 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1, -2
Deflection Temperature at 0.46 MPa (66 psi) 127 °C261 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 104 °C219 °FISO 75-1,-2
Vicat Softening Point 126 °C
@Load 5.10 kg
259 °F
@Load 11.2 lb
120°C/h; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 °C500 °FInjection; ISO 294
Mold Temperature 80.0 °C176 °FInjection; ISO 294

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical LUPOY EC5000A PC/ABS
Covestro Bayblend® M301 FR PC/ABS Blend
Covestro Bayblend® M850 XF PC/ABS Blend
Covestro Bayblend® M303 FR PC/ABS Blend
Covestro Bayblend® T90 XF PC/ABS Blend

PCOVEST0054 / 201837

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.