MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SK Chemicals SARAN™ 560-CX Vapor Retarder Film  (discontinued **)
Categories: Polymer; Adhesive; Film

Material Notes: SARAN™ 560-CX Vapor Retarder Film is composed of a film of the barrier polymer polyvinylidene chloride (PVDC) coextruded with other specialty polymers that provide strength and support. Working together, the portions of this coextruded film combine to create a vapor retarder and jacketing material for mechanical insulation systems that is durable, flexible and has excellent resistance to water vapor penetration. Designed specifically for high vapor drive applications, SARAN 560-CX Film helps prevent water absorption and strongly resists moisture vapor drive into the insulation. A permeance rating of 0.01 perms meets or exceeds the strictest industry requirements for vapor retarders in cold service. SARAN 560-CX Vapor Retarder Film is not a known nutrient source for mold or mildew.

Applications: SARAN 560-CX Vapor Retarder Film is a high-performance, cost effective vapor retarder used in many pipe insulation applications. Typical applications for SARAN 560 CX Film include:

  • Food and beverage facilities
  • Chilled water piping and HVAC systems
  • Transport pipelines
  • Chemical condensation tanks
  • Cold storage systems
  • Refrigerated transport
  • Pharmaceutical plants
  • Petrochemical plants
  • Cryogenic systems, including liquefied natural gas (LNG)

SK Global Chemical has purchased the SARAN® resin business from Dow.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Vapor Transmission 0.0420 g/100 in²/day
@Temperature 37.8 °C
90% RH; ASTM F1249
Thickness 6.00 milASTM D374
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 1960 psiUltimate; ASTM D882
Film Tensile Strength at Yield, TD 1820 psiUltimate; ASTM D882
Film Elongation at Yield, MD 228 %Ultimate; ASTM D882
Film Elongation at Yield, TD 150 %Ultimate; ASTM D882
2% Secant Modulus 70500 psiTD; ASTM D822
 70800 psiMD; ASTM D822
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 121 °C
Minimum Service Temperature, Air -40.0 °C
Flame Spread Index 25ASTM E84
Shrinkage >= 1.0 %
@Temperature 100 °C
Unrestrained, Air, MD
 >= 1.0 %
@Temperature 100 °C
Unrestrained, Air, TD
 
Descriptive Properties
ColorWhite
Mullen Burst Strength83 lbs/in²ASTM D774
Permeance0.01ASTM E96
Surface Burning Characteristics50Smoke Developed, ASTM E84
Ultimate Tensile Strength11 lb/inwidth, TD, ASTM D882
 12 lb/inwidth, MD, ASTM D882
Yield26.1 ft²/lb

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SK Chemicals Saran® 560 Vapor Retarder Film
SK Chemicals SARAN™ 560 CX Vapor Retarder Tape
SK Chemicals Saran® 560 Clear Plastic Barrier Film
Elliott Company ELFOAM® P200 Polyisocyanurate Foam
Tin, Sn

PITWZ003 / 187069

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.