MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® HexWeb® HRH-10/F50 - 5.0 Nonmetallic Flex-Core Honeycomb
Categories: Other Engineering Material; Composite Fibers; Polymer; Thermoset; Aramid; Phenolic

Material Notes: Designation: Material/Cell Size (cells per lineal foot in W direction)-Density
Hexcel manufactures two types of nonmetallic reinforced plastic HexWeb® Flex-Core®: HexWeb® HRP - Fiberglasses cloth reinforced with a high temperature phenolic resin. This product provides good retention of strength for temperatures up to 350°F.
HexWeb® HRH-10 - NOMEX® aramid paper reinforced with a high temperature phenolic resin. This product provides good retention of strength for temperatures up to 300°F.

Features: Specifically designed for formability; Retains mechanical properties in the curved condition; Offers cost savings for curved panels.
Applications: The HexWeb® Nonmetallic Flex-Core® cell configuration as opposed to the standard hexagonal cell honeycomb provides for exceptional formability into compound curvatures with reduced anticlastic curvature and controlled buckling of cell walls. When formed into tight radii, HexWeb® Nonmetallic Flex-Core® provides higher shear strengths than comparable hexagonal cores of equivalent density. HexWeb® Nonmetallic Flex-Core® applications exist wherever extreme curvature dictates a flexible cell geometry, e.g. radomes, ducts, leading edges of wings and stabilizers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 5.00 lb/ft³
 
Mechanical PropertiesOriginal ValueComments
Compressive Yield Strength >= 0.520 ksiBare, min
 >= 0.540 ksiStabilized, min
 0.670 ksiBare, typical
 0.690 ksiStabilized, typical
Shear Modulus 5.20 ksiPlate Shear, W Direction, typical
 10.0 ksiPlate Shear, L Direction, typical
Shear Strength >= 0.170 ksiPlate Shear, W Direction, min
 0.215 ksiPlate Shear, W Direction, typical
 >= 0.300 ksiPlate Shear, L Direction, min
 0.380 ksiPlate Shear, L Direction, typical
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 300 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexWeb® HRH-36® Flex-Core® HRH-36 - F50 - 3.5 Aramid Honeycomb
Solvay Thornel® Mat VMC Carbon Fiber
EconCore ThermHex THPP60-FN Polypropylene Honeycomb Core Sheet
EconCore ThermHex THPP120-FN Polypropylene Honeycomb Core Sheet
DuPont™ Nomex® N196 Paper, 7 mil Nominal Thickness

PHEXC384 / 98855

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.