MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Epoxy Technology EPO-TEK® 375 High Temperature Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy, High Temperature

Material Notes: Product Description: EPO-TEK®375 is a two component, high temperature epoxy designed for semiconductor, hybrid, fiber optic, and medical applications. Also available in a single component frozen syringe.

Advantages & Application Notes:

  • Reasonable pot-life that allows for low temperature curing to be realized. It has an amber color change upon cure.
  • Semiconductor suggested applications: wafer-wafer bonding of CSP; fabrication of MEMs devices; flip chip underfill.
  • Hybrid suggested applications: providing near hermetic seals and UHV seals in sensor devices and resisting high temperature packaging.
    • Down-hole petrochemical fiber optic sensors resisting >200°C field conditions.
  • Fiber optic adhesive suggested applications:
    • Sealing fiber into ferrules, transmitting light in the optical pathway from 800- 1550 nm range.
    • Fiber component packaging, adhesive for active alignment of optics, environmental seal of opto-package, V-groove arrays.
  • Medical suggested applications:
    • Potting fiber optic bundles into ferrules for light guides and endoscopes; capable of resisting several sterilization techniques including ETO, gamma, ION beam, H202 plasma, and >200 autoclave steam cycles; excellent adhesion to surfaces including stainless steel, diamond, titanium, brass, ceramics, glass and most plastics.
    • Certified to USP Class VI Biocompatibility Standards for medical implants; adhesive for catheter devices including stents and guide wires.
  • Electronics Assembly suggested applications:
    • Used as dielectric layer in the fabrication of capacitors; laminating PZT ferroelectrics found in ultrasound or ink-jetting devices.
    • Impregnating and insulating copper coil windings in motors and inductor coils. Bonding ferrite cores and magnets.
    • Structural grade epoxy found in hard-disk drive devices; bonding of stainless steel metals, kapton, and magnets.

Information Provided by Epoxy Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.00 g/ccPart B
 1.20 g/ccPart A
Viscosity 3000 - 5000 cP
@Temperature 23.0 °C
50 rpm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 88
Tensile Modulus 339000 psiStorage
Shear Strength >= 2000 psiLap
 >= 3400 psiDie
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cm
Dielectric Constant 3.34
@Frequency 1000 Hz
Dissipation Factor 0.0040
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 48.0 µm/m-°CBelow Tg
 192 µm/m-°CAbove Tg
Maximum Service Temperature, Air 200 °CContinuous
 300 °CIntermittent
Minimum Service Temperature, Air -55.0 °CContinuous
 -55.0 °CIntermittent
Glass Transition Temp, Tg >= 100 °CDynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min
Decomposition Temperature 421 °CDegradation Temperature
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.5692
@Wavelength 589 nm
Transmission, Visible >= 94 %
@Wavelength 600 - 790 nm
Spectral
 >= 98 %
@Wavelength 800 - 1500 nm
Spectral
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 min
@Temperature 150 °C
Minimum Bond Line
 20.0 min
@Temperature 120 °C
Minimum Bond Line
 60.0 min
@Temperature 100 °C
Minimum Bond Line
 90.0 min
@Temperature 80.0 °C
Minimum Bond Line
Pot Life 240 min
Shelf Life 12.0 Month
@Temperature 25.0 °C
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes
 
Descriptive Properties
ColorAmberPart B
 Clear/ColorlessPart A
ConsistencyPourable liquid
Mix Ratio by Weight10:1
Number of ComponentsTwo
Weight Loss0.06%200°C
 0.16%250°C
 0.49%300°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® 353ND High Temperature Epoxy
Cotronics Resbond™ 954 High Temperature Ceramic Adhesive, Stainless Steel Composition
Epoxy Technology EPO-TEK® 337H Graphite-Filled, High Temperature Epoxy
Epoxy Technology EPO-TEK® 377 High Temperature Epoxy
Epoxy Technology EPO-TEK® 383ND High Temperature Epoxy

PPOXYT131 / 141170

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.