MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo Plexiglas® V052i Acrylic
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Heat Resistant, Molded

Material Notes: Plexiglas® V052i is an impact modified thermoplastic acrylic resin formulated for injection molding. It is characterized by its chemical and heat resistance as well a good melt flow and excellent mold release properties. It has higher impact strength than Plexiglas® V052 for improved fabrication. It offers an excellent balance between melt flow and increased resistance to breakage, while providing weatherability superior to that provided by other high-impact plastics. Moldflow simulation data is available.

Appearance: Clear/Transparent; Colors Available; Opaque; Translucent

Characteristics: High Clarity; High Scratch Resistance; Good Color Stability, Good Dimensional Stability; Low Shrinkage; Good Thermal Stability, Good UV Stability; Medium Heat Resistance; Good Weather Resistance

Applications: Automotive Applications; Consumer Applications

Arkema has sold the American Plexiglas® product line to Trinseo, finalized in 2021.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.18 g/ccASTM D792
Water Absorption 0.40 %24 hr. immersion; ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cmASTM D955
Melt Flow 3.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 84ASTM D785
Tensile Strength, Ultimate 9200 psiASTM D638
Elongation at Break 22 %ASTM D638
Tensile Modulus 410000 psiASTM D638
Flexural Strength <= 14000 psiASTM D790
Flexural Modulus 420000 psiASTM D790
Izod Impact, Notched 0.400 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 1.30 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 217 °Fannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 207 °Fannealed; ASTM D648
Vicat Softening Point 203 °F50°C/hr; 10N; ASTM D1525
 216 °F50°C/hr; 50N; ASTM D1525
Flammability, UL94 HB
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.49
@Temperature 22.8 °C
ND; ASTM D542
Haze <= 1.0 %
@Thickness 3.17 mm
ASTM D1003
Transmission, Visible 91 %
@Thickness 3.17 mm
ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo Plexiglas® V052 Acrylic
LG Chemical Lupoy 1303EP-22 Polycarbonate Resin
DuPont Mobility and Materials Zytel® FR70G25V0 BK369 PA66-GF25FR(17)
LG Chemical HI835M PMMA, Impact Resistant Grade
Envalior Novamid® 3010GN30 NAT PA66-GF30 FR(17)

PARKG028 / 24382

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.