MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ConocoPhillips Hydroclear® 6 Ultra-Clean Spindle Oil
Categories: Fluid; Lubricant

Material Notes: Description: Conoco Hydroclear Ultra-Clean Spindle fluids comprise blends of special base oils and additives specially formulated for use in applications where a lubricant combining the properties of a light spindle oil and light hydraulic oil are required.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012, and branding was further reorganized in 2016. The Hydroclear® trade name is no longer in use but products may be available under different names.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.833 g/ccASTM D-4052
API Gravity 38.4 °ASTM D-1298
Kinematic Viscosity 8.5 cSt
@Temperature 21.0 °C
ASTM D 445
Kinematic Viscosity at 40°C (104°F) 5.07 cStASTM D 445
Kinematic Viscosity at 100°C (212°F) 1.72 cStASTM D 445
ASTM Color <= 0.50
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 0.010mg KOH/g; ASTM D-974
 
Mechanical PropertiesOriginal ValueComments
Coefficient of Friction 0.043ASTM D4172A
Four Ball Wear 0.193 mmScar Diameter; ASTM D-4172A
 
Thermal PropertiesOriginal ValueComments
Pour Point -40.0 °FASTM D-97
Flash Point 300 °FASTM D-92
 
Descriptive Properties
Copper Corrosion1AASTM D130
Emulsion Characteristics (40-40-0)10 minutesASTM D-1401
Freshwater Rust TestPassASTM D665A
ISO Cleanliness Code14/11Applies to packaged goods only.
Sim. Seawater Rust TestPassASTM D665B
Thermal Stability4 mg/100 mLMod. CM "A" Sludge

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON139 / 75176

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.