MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Precision Polymer Engineering F50A Fluorosilicone Rubber
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE); Silicone

Material Notes: Blue Fluorosilicone, 45-55 °IRHD. Fluorosilicone rubber having methyl, vinyl and fluorine substituent groups on the polymer chain.

Applications: Excellent heat resistance and low temperature flexibility. Suitable for sealing petroleum oils and hydrocarbon fuels. Fluorosilicones are widely used in aircraft fuel systems.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 50°IRHD; ASTM D1415
Tensile Strength, Yield 7.50 MPaASTM D412
Elongation at Break 300 %ASTM D412
Compression Set 10 %
@Temperature 150 °C,
Time 79200 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 250 °C
Minimum Service Temperature, Air -60.0 °C
 -55.0 °CASTM D2137, Non-brittle after 3 minutes
Flash Point >= 300 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Fluorosilicone Rubber (FMQ, FVMQ, FSi)
Dow Silastic® LS 4-9038 FLUOROSILICONE RUBBER
Dow Silastic® LS 5-2040 FLUOROSILICONE RUBBER
ATG s.r.l. FVMQ Fluorosilicone Rubber
Applied Silicone 40130 Fluorosilicone Barrier Dispersion, Implant Grade

PPRECI137 / 57861

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.