MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Surlyn® 8940 Ionomer Resin, Sodium
Categories: Polymer; Thermoplastic; Ionomer; Ionomer, Molded

Material Notes: Surlyn® 8940 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neutralization levels for this grade are optimized to deliver excellent clarity and high stiffness compared with other grades of Surlyn®. The resin can be injection molded, and is processable by extrusion into sheets or shapes. It complies with the provisions of U.S. Food and Drug Administration (FDA) Title 21 Code of Regulations 177:1330 - ionomer resins.

Data provided by the manufacturer.

This former DuPont product line is now a Dow product line.

Key Words: Ethylene/Methacrylic Acid (E/MAA) Copolymer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/ccASTM D792
Melt Flow 2.8 g/10 min
@Load 2.16 kg,
Temperature 190 °C
condition E; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65ASTM D2240
Tensile Strength, Ultimate 33.0 MPaASTM D638
Tensile Strength, Yield 15.0 MPa50 mm/min cross speed; ASTM D638
Elongation at Break 470 %ASTM D638
Flexural Modulus 0.350 GPaASTM D790
Izod Impact, Notched 10.25 J/cmASTM D256
Tensile Impact Strength 1020 kJ/m²ASTM D1822S
Tear Strength 148 kN/mDie C; ASTM D624
Abrasion 370NBS Index; ASTM D1630
 
Thermal PropertiesOriginal ValueComments
CTE, linear 100 µm/m-°C
@Temperature -20.0 - 32.0 °C
ASTM D696
Thermal Conductivity 0.246 W/m-K
Melting Point 94.0 °CDSC
Deflection Temperature at 0.46 MPa (66 psi) 44.0 °CASTM D648
Vicat Softening Point 63.0 °CRate B, ASTM D1525-70
Brittleness Temperature -106 °CASTM D746
Flame Spread 22.9 mm/minASTM D635
 
Optical PropertiesOriginal ValueComments
Haze 5.0 %
@Thickness 6.40 mm
ASTM D1003A
Gloss 50 %20° per ASTM D523-6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Surlyn® PC100 Ionomer Resin, Highest Clarity, Sodium
Dow Surlyn® 2601B Sodium Ionomer
Dow Surlyn® 1605 Sodium Ionomer Resin for Blown/Cast Film and Extrusion Coating
Dow Surlyn® 1707 Sodium Ionomer
Dow Surlyn® 8150 Ionomer Resin, Sodium

PDU411 / 33062

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.