MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Wacker Wacker® AK 200000 Silicone Fluid
Categories: Fluid; Polymer; Thermoset; Silicone

Material Notes: Product description: WACKER® AK 200 000 is a linear, non-reactive polydimethylsiloxane with a viscosity of approx. 200 000 mm²/s. Due to its chemical structure, WACKER® AK 200 000 has an outstanding property profile, which sets it apart from organic materials such as mineral oils.

Properties: WACKER® AK 200 000 is a clear, odorless and colorless liquid.

Special features:

  • minimal change in physical properties over a broad temperature range
  • excellent water-repellent properties
  • good dielectric properties
  • low surface tension and thus high surface activity
  • chemically highly unreactive
  • low solidifying point
  • high flash point
  • high heat resistance
  • good solubility in a wide range of solvents
Application:
  • antifoam agent
  • liquid dielectric for electrical and electronic equipment
  • plastics additive
  • damping medium
Silicone fluids from the BELSIL® line are available for the cosmetic sector. Whenever particularly high heat and shear resistance is required, manufacturer recommends silicone fluids from the AK stab, AK visc and AKC product lines.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.970 g/cc0.0350 lb/in³DIN 51757
Kinematic Viscosity 200000 cSt200000 cStDIN 53019
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 320 °C>= 608 °FISO 2592
Ignition Temperature 450 °C842 °FDIN 51794
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4041.404
Transmission, Visible 90 %90 %"Clear" but manufacturer does not quantify.
 
Descriptive Properties
Appearancecolorless, clear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWACK9722 / 205251

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.