MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Washington Penn Medium Impact Copolymer 30% Talc Filled
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Talc Filler

Material Notes: Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requirements. These products have excellent mold detail and surface reproduction with fast set-up times. They are also available in an array of colors.

Information provided by Washington Penn Plastic Co.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccASTM D792
Filler Content 30 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 3400 psiASTM D638
Elongation at Break 40 %ASTM D638
Elongation at Yield 7.0 %ASTM D638
Flexural Modulus 385 ksiTangent; ASTM D790
Flexural Modulus, 1% Secant 310 ksiASTM D790
Izod Impact, Notched 1.00 ft-lb/inASTM D256
Gardner Impact 49.0 in-lb
@Temperature -30.0 °C
ASTM D5420
 122 in-lb
@Temperature 23.0 °C
ASTM D5420
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 250 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Washington Penn Homopolymer Polypropylene 30% Talc Filled
Washington Penn Homopolymer Polypropylene 20% Talc Filled
A. Schulman POLYFORT™ FPP 2121UV-M-31 Black Filled Polypropylene Homopolymer
LyondellBasell Astryn 65F4-3 Polypropylene Homopolymer, 30% Talc
LyondellBasell Astryn 75F4-2 Polypropylene Copolymer, 20% Talc

PWPP43 / 72826

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.