MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Freudenberg Hydrolysis-Resistant Polyurethane Elastomer
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced; Rubber or Thermoset Elastomer (TSE)

Material Notes: Developed for the Drinking Water Sector. Free of plasticisers. With hydrolysisresistant polyurethanes which have been specially developed with drinking water applications in mind, Simrit is now offering an interesting alternative to conventional materials which features many benefits, including Excellent wear resistance, Highly adjustable hardness range; Good tensile strength and breaking elongation; Resistance to mineral oils in wide temperature ranges; High ozone and oxidation resistance; Excellent damping behaviour; Enormous resistance to crack formation and crack growth.

Information provided by Freudenburg-NOK.

This product was formerly sold under the Freudenberg Simrit division; now Freudenberg Sealing Technologies.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 85 - 94

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Scotchkote™ 60EG 533 Urethane Elastomer
Northstar Polymers GK-7 Low Viscosity Polyurethane Gel Cast
Northstar Polymers MPC-W44A Polyurethane Gel
Northstar Polymers SAI-1 Low Viscosity Variable Ratio Polyurethane Gel
Resinlab® UR3001 Clear Two Part Urethane Encapsulant

PSIMR030 / 67734

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.