MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Polycarbonate/ASA Alloy, Unreinforced
Categories: Polymer; Thermoplastic; ASA Polymer; Polycarbonate (PC); Polycarbonate/ASA Alloy, Unreinforced

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 - 1.24 g/cc0.0387 - 0.0448 lb/in³Average value: 1.15 g/cc Grade Count:90
Water Absorption 0.100 - 0.500 %0.100 - 0.500 %Average value: 0.245 % Grade Count:8
Moisture Absorption at Equilibrium 0.150 - 0.350 %0.150 - 0.350 %Average value: 0.210 % Grade Count:13
Water Absorption at Saturation 0.400 - 0.900 %0.400 - 0.900 %Average value: 0.650 % Grade Count:10
Viscosity  225000 - 225000 cP
@Temperature 260 - 260 °C
225000 - 225000 cP
@Temperature 500 - 500 °F
Average value: 238000 cP Grade Count:1
 225000 - 225000 cP
@Frequency 1000 - 1000 Hz
225000 - 225000 cP
@Frequency 1000 - 1000 Hz
Average value: 238000 cP Grade Count:1
 251000 - 251000 cP
@Temperature 260 - 260 °C
251000 - 251000 cP
@Temperature 500 - 500 °F
Average value: 238000 cP Grade Count:1
 251000 - 251000 cP
@Shear Rate 1000 - 1000 1/s
251000 - 251000 cP
@Shear Rate 1000 - 1000 1/s
Average value: 238000 cP Grade Count:1
Linear Mold Shrinkage 0.00300 - 0.00900 cm/cm0.00300 - 0.00900 in/inAverage value: 0.00591 cm/cm Grade Count:68
Linear Mold Shrinkage, Transverse 0.00400 - 0.00750 cm/cm0.00400 - 0.00750 in/inAverage value: 0.00578 cm/cm Grade Count:16
Melt Flow 0.700 - 80.0 g/10 min0.700 - 80.0 g/10 minAverage value: 20.7 g/10 min Grade Count:85
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 102 - 118102 - 118Average value: 112 Grade Count:17
Ball Indentation Hardness 85.0 - 120 MPa12300 - 17400 psiAverage value: 104 MPa Grade Count:11
Tensile Strength, Ultimate 42.7 - 65.0 MPa6190 - 9430 psiAverage value: 54.5 MPa Grade Count:39
Tensile Strength, Yield 41.0 - 65.0 MPa5950 - 9430 psiAverage value: 56.0 MPa Grade Count:67
Elongation at Break 3.00 - 110 %3.00 - 110 %Average value: 49.2 % Grade Count:52
Elongation at Yield 2.70 - 40.0 %2.70 - 40.0 %Average value: 7.61 % Grade Count:30
Modulus of Elasticity 1.86 - 3.10 GPa270 - 450 ksiAverage value: 2.32 GPa Grade Count:33
Flexural Yield Strength 63.8 - 100 MPa9250 - 14500 psiAverage value: 82.4 MPa Grade Count:61
 15.0 - 15.0 MPa
@Temperature 110 - 110 °C
2180 - 2180 psi
@Temperature 230 - 230 °F
Average value: 15.0 MPa Grade Count:1
Flexural Modulus 0.700 - 2.96 GPa102 - 430 ksiAverage value: 2.32 GPa Grade Count:74
Poissons Ratio 0.280 - 0.3600.280 - 0.360Average value: 0.332 Grade Count:5
Izod Impact, Notched 1.18 - 9.08 J/cm2.20 - 17.0 ft-lb/inAverage value: 4.73 J/cm Grade Count:53
 1.1768 - 5.50 J/cm
@Temperature -30.0 - 0.000 °C
2.2046 - 10.3 ft-lb/in
@Temperature -22.0 - 32.0 °F
Average value: 1.65 J/cm Grade Count:5
 0.374 - 1.96133 J/cm
@Temperature -30.0 - -30.0 °C
0.701 - 3.67438 ft-lb/in
@Temperature -22.0 - -22.0 °F
Average value: 1.65 J/cm Grade Count:7
 0.374 - 1.96133 J/cm
@Thickness 3.17 - 6.40 mm
0.701 - 3.67438 ft-lb/in
@Thickness 0.125 - 0.252 in
Average value: 1.65 J/cm Grade Count:7
Izod Impact, Notched (ISO) 10.0 - 60.0 kJ/m²4.76 - 28.6 ft-lb/in²Average value: 39.1 kJ/m² Grade Count:25
 6.00 - 38.0 kJ/m²
@Temperature -30.0 - -20.0 °C
2.86 - 18.1 ft-lb/in²
@Temperature -22.0 - -4.00 °F
Average value: 16.1 kJ/m² Grade Count:12
Izod Impact, Unnotched (ISO) NB - NB
@Temperature -30.0 - -30.0 °C
NB - NB
@Temperature -22.0 - -22.0 °F
Grade Count:1
Charpy Impact Unnotched 9.00 J/cm² - NB42.8 ft-lb/in² - NBAverage value: 9.00 J/cm² Grade Count:8
 999.9 - 999.9 J/cm²
@Temperature -30.0 - -30.0 °C
4759 - 4759 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Grade Count:2
Charpy Impact, Notched 1.50 - 7.00 J/cm²7.14 - 33.3 ft-lb/in²Average value: 4.38 J/cm² Grade Count:29
 0.600 - 5.50 J/cm²
@Temperature -40.0 - -20.0 °C
2.86 - 26.2 ft-lb/in²
@Temperature -40.0 - -4.00 °F
Average value: 2.06 J/cm² Grade Count:18
Gardner Impact >= 72.3 J
@Temperature -29.0 - -29.0 °C
>= 53.3 ft-lb
@Temperature -20.2 - -20.2 °F
Average value: 72.3 J Grade Count:1
Puncture Energy 38.0 - 45.0 J
@Temperature -30.0 - -30.0 °C
28.0 - 33.2 ft-lb
@Temperature -22.0 - -22.0 °F
Average value: 41.5 J Grade Count:2
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+11 - 1.00e+17 ohm-cm1.00e+11 - 1.00e+17 ohm-cmAverage value: 6.04e+15 ohm-cm Grade Count:20
Surface Resistance 1.00e+11 - 1.00e+16 ohm1.00e+11 - 1.00e+16 ohmAverage value: 1.37e+15 ohm Grade Count:20
Dielectric Constant 2.80 - 3.402.80 - 3.40Average value: 3.06 Grade Count:11
Dielectric Strength 13.1 - 37.0 kV/mm333 - 940 kV/inAverage value: 32.4 kV/mm Grade Count:7
Dissipation Factor 0.00250 - 0.01500.00250 - 0.0150Average value: 0.00757 Grade Count:11
Comparative Tracking Index 175 - 600 V175 - 600 VAverage value: 363 V Grade Count:6
 
Thermal PropertiesMetricEnglishComments
CTE, linear 65.0 - 110 µm/m-°C36.1 - 61.1 µin/in-°FAverage value: 82.6 µm/m-°C Grade Count:17
 72.0 - 80.0 µm/m-°C
@Temperature 40.0 - 100 °C
40.0 - 44.4 µin/in-°F
@Temperature 104 - 212 °F
Average value: 75.7 µm/m-°C Grade Count:3
CTE, linear, Transverse to Flow 70.0 - 115 µm/m-°C38.9 - 63.9 µin/in-°FAverage value: 79.8 µm/m-°C Grade Count:7
 87.0 - 87.0 µm/m-°C
@Temperature 40.0 - 100 °C
48.3 - 48.3 µin/in-°F
@Temperature 104 - 212 °F
Average value: 87.0 µm/m-°C Grade Count:1
Thermal Conductivity 0.170 - 0.190 W/m-K1.18 - 1.32 BTU-in/hr-ft²-°FAverage value: 0.173 W/m-K Grade Count:8
Hot Ball Pressure Test 95.0 - 130 °C203 - 266 °FAverage value: 114 °C Grade Count:4
Deflection Temperature at 0.46 MPa (66 psi) 96.1 - 134 °C205 - 273 °FAverage value: 117 °C Grade Count:38
Deflection Temperature at 1.8 MPa (264 psi) 76.0 - 122 °C169 - 252 °FAverage value: 103 °C Grade Count:69
Vicat Softening Point 96.0 - 146 °C205 - 295 °FAverage value: 124 °C Grade Count:66
Flammability, UL94 HB - V-0HB - V-0Grade Count:49
Glow Wire Test 650 - 960 °C1200 - 1760 °FAverage value: 787 °C Grade Count:17
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 216 - 277 °C420 - 530 °FAverage value: 251 °C Grade Count:12
Melt Temperature 199 - 300 °C390 - 572 °FAverage value: 254 °C Grade Count:40
Mold Temperature 26.7 - 100 °C80.0 - 212 °FAverage value: 70.3 °C Grade Count:40
Injection Velocity 200 - 240 mm/sec7.87 - 9.45 in/secAverage value: 213 mm/sec Grade Count:12
Drying Temperature 79.4 - 110 °C175 - 230 °FAverage value: 94.6 °C Grade Count:38
Moisture Content 0.0200 - 0.100 %0.0200 - 0.100 %Average value: 0.0423 % Grade Count:13

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
Overview of materials for ASA/AES, Unreinforced, Extruded/Molded
INEOS Styrolution Luran® S 778T ASA
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced
LG Chemical LI912 ASA

O3179a / 89082

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.