MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Zytel® 70G50HSLA BK039B PA66-GF50
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 50% Glass Fiber Filled

Material Notes: 50% Glass Reinforced, Heat Stabilized, Polyamide 66

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.57 g/ccDAM; ISO 1183
Melt Density 1.40 g/cc
@Temperature 295 °C
Water Absorption 4.2 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
 0.80 %
@Thickness 2.00 mm,
Time 86400 sec
Immersion; DAM; Sim. to ISO 62
Moisture Absorption 1.20 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Viscosity Number 105 cm³/g96% sulfuric acid; ISO 307, 1157, 1628
Linear Mold Shrinkage, Flow 0.0030 cm/cmDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cmDAM; ISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 300 MPaH 961/30; DAM; ISO 2039-1
Tensile Strength at Break 170 MPa50% RH; ISO 527-1/-2
 240 MPaDAM; ISO 527-1/-2
Elongation at Break 2.4 %DAM; ISO 527-1/-2
 3.5 %50% RH; ISO 527-1/-2
Tensile Modulus 13000 MPa50% RH; ISO 527-1/-2
 17000 MPaDAM; ISO 527-1/-2
Flexural Strength 280 MPa50% RH; ISO 178
 400 MPaDAM; ISO 178
 270 MPa
@Strain 3.5 %
50% RH; ISO 178
Flexural Modulus 12000 MPa50% RH; ISO 178
 16000 MPaDAM; ISO 178
Compressive Strength 215 MPaDAM; ISO 604
Poissons Ratio 0.3350% RH
 0.33DAM
Shear Strength 90.0 MPaDAM; ASTM D 732
Charpy Impact Unnotched 90.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 90.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 90.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
 95.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
Charpy Impact, Notched 14.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 15.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 15.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 20.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
Puncture Energy 10.0 J
@Temperature 23.0 °C
DAM; ISO 6603-2
Tensile Creep Modulus, 1 hour 10000 MPa1h; 50% RH; ISO 899-1
Tensile Creep Modulus, 1000 hours 8000 MPa1000h; 50% RH; ISO 899-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmDAM; IEC 62631-3-1
Surface Resistance 4.00e+14 ohm50% RH; IEC 62631-3-2
Dielectric Strength 30.0 kV/mmDAM; IEC 60243-1
Comparative Tracking Index 500 VDAM; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 9.00 µm/m-°CDAM; ISO 11359-1/-2
 13.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
DAM; ISO 11359-1/-2
 19.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
DAM; ASTM E 831
 19.0 µm/m-°C
@Temperature 55.0 - 160 °C
DAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 72.0 µm/m-°CDAM; ISO 11359-1/-2
 42.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
DAM; ISO 11359-1/-2
 61.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
DAM; ASTM E 831
 114 µm/m-°C
@Temperature 55.0 - 160 °C
DAM; ISO 11359-1/-2
Specific Heat Capacity 1.87 J/g-°C
@Temperature 295 °C
Melt
Thermal Conductivity 0.460 W/m-KSolid
 0.310 W/m-K
@Temperature 295 °C
Melt
Melting Point 262 °C10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 261 °CDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 255 °CDAM; ISO 75-1/-2
Vicat Softening Point 255 °C50°C/h, 50N; DAM; ISO 306
Glass Transition Temp, Tg 20.0 °C10°C/min; 50% RH; ISO 11357-1/-2
 65.0 °C10°C/min; DAM; ISO 11357-1/-2
Flammability, UL94 HB
@Thickness 0.830 mm
DAM; IEC 60695-11-10
 HB
@Thickness 1.50 mm
DAM; IEC 60695-11-10
Oxygen Index 24 %DAM; ISO 4589-1/-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 295 °COptimum, Injection
 285 - 305 °CRange, Injection
Mold Temperature 70.0 - 120 °CInjection
 100 °COptimum, Injection
Ejection Temperature 210 °CInjection
Drying Temperature 80.0 °CInjection
Dry Time 2.00 - 4.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.20 %Injection
Hold Pressure 50.0 - 100 MPaRange, Injection
 
Descriptive Properties
AdditivesRelease agent
Drying RecommendedyesInjection
Emission of organic compounds (µgC/g)6.5VDA 277
FMVSS ClassSEISO 3795 (FMVSS 302)
Fogging (mg)0.4G-value (condensate); ISO 6452; DAM
ISO designationISO 16396-PA66,GF50,M1CGHR,S10-160
Max. screw tangential speed (m/s)0.2Injection
Odor Class3VDA 270
Part Marking Code>PA66-GF50<ISO 11469
PolymerPA66-GF50
Processing Hold Pressure Time (s/mm)3Injection
Resin IdentificationPA66-GF50ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Zytel® FG70G50HSLA BK309 PA66-GF50
Celanese Zytel® 70G35HSLRA4 BK267 PA66-GF35
Asahi Kasei Thermylon® NSG-240A 50% Ceramic and Glass Fiber Reinforced Nylon 6
Celanese Zytel® 73G50HSLA BK416 PA6-GF50
Celanese Zytel® 101 NC010 PA66

PDSX5343 / 197983

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.