MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Copper Alloy, UNS C89940, M01 Temper, As Sand Cast
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: As Sand Cast

Casting Characteristics: High – Gassing; Medium – Drossing, Casting Yield, Effect of Section Size, Fluidity, Shrinkage in Solidification

Fabrication Properties: Excellent Suitability – Soldering

Typical uses: Bearings; Gears for Ice Cream Pumps; Mold Plates for Food Shape Machines; Plungers for Food Shape Machines

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.320 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 120
@Load 500 kg
Tensile Strength 25.0 ksi
Tensile Strength, Yield 24.0 ksi0.2% Offset
Elongation at Break 2.5 %
Compressive Strength 24.0 ksi0.1 in. set/in.
Machinability 30 %
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.70 µin/in-°F
@Temperature 20.0 - 300 °C
Thermal Conductivity 14.36 BTU-in/hr-ft²-°F
Melting Point 1978 - 2145 °F
Solidus 1978 °F
Liquidus 2145 °F
Shrinkage 1.56 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Processing PropertiesOriginal ValueComments
Processing Temperature 950 °FStress Relief
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.0050 %
Antimony, Sb <= 0.10 %
Bismuth, Bi 4.0 - 5.5 %
Copper, Cu 64 - 68 %
Iron, Fe 0.70 - 2.0 %
Lead, Pb <= 0.010 %
Manganese, Mn <= 0.20 %
Nickel, Ni 20 - 23 %
Phosphorus, P 0.10 - 0.15 %
Silicon, Si <= 0.15 %
Sulfur, S <= 0.050 %
Tin, Sn 3.0 - 5.0 %
Zinc, Zn 3.0 - 5.0 %
 
Descriptive Properties
Proportional Limit20 ksi
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC89940x1 / 292603

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.